Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (2): 79-158    DOI:
Current Issue | Archive | Adv Search |
THE OPTICAL CONSTANTS OF SULPHIDES
WU Weitao (Institute of Metal Research; Academia Sinica; Shenyang); Irfan AYDIN; Hans-Eugen BUHLER (Dechema-Institut; Frankfurt/M.)
Cite this article: 

WU Weitao (Institute of Metal Research; Academia Sinica; Shenyang); Irfan AYDIN; Hans-Eugen BUHLER (Dechema-Institut; Frankfurt/M.). THE OPTICAL CONSTANTS OF SULPHIDES. Acta Metall Sin, 1983, 19(2): 79-158.

Download:  PDF(5523KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  For the first time the optical constants of different sulphides were measuredusing interference layer microscopy to enable them to be utilized for quantitativemetallography. In addition to the measurement of the refractive index and absorp-tion coefficient it was also possible to give the conditions that enable the maximumpossible light-dark contrast as well as a good colour contrast to be achieved in thepolished specimen. The layer materials that almost completely extinguish thereflectivity of the different phases are reported together with the exact colouraccording to DIN 6164. A method of presentation was found for all phases, notonly the sulphides, that enabled the refractive index at which the amplitudecondition was fulfilled to be exactly determined. There is a mathematical relation-ship that can be simply derived for all phases between the reflectivity at theinterference minimum of a phase and the refractive index of the layer providingnon-absorbent layer materials are used.The sulphides represent a very complicated phase group for the metallographer as the amplitude condition can be over- or under- fulfilled by coating with the layer materials under discussion e.g. ZnS or ZnSe. One of the aims of this work was to provide the necessary data.
Received:  18 February 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I2/79

1 Aydin, I; Buehler, H.-E.; Rahmel, A., Proc. 13th Annual Meeting IMS, Ed. Petzow, G., Brighton, 1980.
2 Buehler, H.-E; Hougrardy, H.-P., Atlas der Interferenzschichten-Metallographie, Deutsche Gesellschaft fuer Metallkunde, Oberursel, 1979.
3 Landolt, H. H.; Boernstein, R., Landolt-Boernstein Zahlenwerte und Funktionen aus Naturwissenschaften und Technik, Neue Serie Gruppe Ⅲ, Bd. 6, Eds. Hellwege, K.-H.; Hellwege, A. M., Springer-Verlag, Berlin, 1971.
4 Buehler, H.-E.; Jackel, G., Arch. Eisenhuettenwes., 41 (1970) , 859.
5 Aydin, I; Buehler, H.-E., Prakt. Metallogr., 17 (1980) , 441.
6 Pepperhoff, W.; Ettwig, H.-H., Interferenzschichten-Mikroskopie, Dr. D, Steinkopf-Verlag, Darmstadt, 1970.
7 Zogg, H.; Weber, S.; Warlimont, H., Prak. Metallogr., 14 (1977) , 553.
8 Buehler, H.-E.; Kossel, D., Prak. Metallogr., Sonderband 12, Dr. Riederer Verlag GmbH, Stuttgart, 1981, p. 27.
9 Jackel, G.; Buehler, H.-E.; Robuch, G., Thyssenforschung, (1972) , №. 4, 67.
10 Buehler, H.-E.; Jackel, G.; Thiemann, E., Arch. Eisenhuettenwes., 41 (1970) , 405.
11 Kossel, D., 私人通讯.
12 Aydin, I.; Buehler, H.-E., Merkblaetter zur Anwendung der Interferenzschichten,待发表.
13 Pauling, L., Nature of the Chemical Bond and the Structure of Molecules and Crystals, 3rd ed., Ithaca, 1960.
14 Buehler, H.-E., Radex-Rundschau, (1975) , № 3, 464.
15 Wu Weitao; Rahmel, A.; Schorr, M., Oxid. Met., to be published.l
No related articles found!
No Suggested Reading articles found!