A NOTE ON BEHAVIOUR OF NON-LINEAR DEPENDENCE OF LOW FREQUENCY LOSS UPON FREQUENCY FOR AMORPHOUS ALLOYS
ZHANG Yanzong (Shanghai Iron and Steer Research Institute) (Manuscript received 24 February; 1983; revised manuscript 5 July; 1983)
Cite this article: 

ZHANG Yanzong (Shanghai Iron and Steer Research Institute) (Manuscript received 24 February; 1983; revised manuscript 5 July; 1983). A NOTE ON BEHAVIOUR OF NON-LINEAR DEPENDENCE OF LOW FREQUENCY LOSS UPON FREQUENCY FOR AMORPHOUS ALLOYS. Acta Metall Sin, 1984, 20(3): 214-220.

Download:  PDF(526KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The behaviour of non-linear dependence of low frequency loss upon frequency has been approached on the basis of the analysis of low frequency loss curves for two types of amorphous alloy. The loss curves were analyzed and calculated by introducing two non-linear losses: the thermal fluctuation magnetic after effect and the micro-eddy current loss. The results show that the non-linearity is mainly attributed to a thermal fluctuation magnetic after effect and a numerical variation of the magnetic domain with frequency.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/214

1 佐佐木堂;桂川茂彦,电气学会论文志,97-A(1977) ,601.
2 Sasaki, T; Hosoe, H., IEEE Trans. Magn., MAG-14 (1978) , 779.
3 Fujimori, H.; Yoshimoto, H.; Masumoto, T., J. Appl. Phys., 52 (1981) , 1893.
4 Washko, S.D.; Osborn, M.L.; Veeraraghaven, W.G., ibid., 52 (1981) , 1899.
5 Sakaki, Y., IEEE Trans. Magn., MAG-16 (1980) , 569.
6 Ferrari, G., Portesell, J. L.; Vergne, R., ibid., MAG-14 (1978) , 764.
7 Ne'el, L., J. Phys. Radium, 11 (1950) , 49.
8 Haller, T. R.; Kramer, J. J., J. Appl. Phys., 41 (1970) , 1034.
9 Pry, R. H.; Bean, C. P., ibid., 29 (1958) , 532.
10 Haller, T. R.; Kramer, J.J., ibid., 41 (1970) , 1036.
11 Sharp, M.R.G.; Horner, J.T., J. Phys. D: Appl. Phys., 6 (1973) , 1835.
12 Mohri, K.; Satoh, Y.; Fujimoto, T., IEEE Trans, Magn., MAG-12 (1976) , 849.
13 29 (1970) , 770.
14 郭贻诚,铁磁学,高等教育出版社,北京,1965,p.355.
15 北京大学物理系,铁磁学编写组,铁磁学,科学出版社,北京,1976年,p.211.
16 Sakaki, Y.; Imagi, I., IEEE Trans. Magn., MAG-17 (1981) , 1478.
17 张延忠,科学通报(待发表).
No related articles found!
No Suggested Reading articles found!