Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (3): 221-291    DOI:
Current Issue | Archive | Adv Search |
EFFECTS OF IONITRIDING ON STRUCTURE OF NITRIDED LAYER AND SUBSTRATE TO Ti AND Ti-6A1-4V ALLOY
ZHANG Lixin; LI Liguang (Institute of Metal Research; Academia Stnica; Shenyang); PENG Hongzhen; WANG Jiuying (Shenyang Institute of Metallurgy)(Manuscript received 2 April; 1983; revised manuscript 17 October; 1983)
Cite this article: 

ZHANG Lixin; LI Liguang (Institute of Metal Research; Academia Stnica; Shenyang); PENG Hongzhen; WANG Jiuying (Shenyang Institute of Metallurgy)(Manuscript received 2 April; 1983; revised manuscript 17 October; 1983). EFFECTS OF IONITRIDING ON STRUCTURE OF NITRIDED LAYER AND SUBSTRATE TO Ti AND Ti-6A1-4V ALLOY. Acta Metall Sin, 1984, 20(3): 221-291.

Download:  PDF(5197KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structures of the nitrided layer and the substrate to commercially pure Ti and Ti-6Al-4V alloy after ionitrided at 750—920℃ have been examined by X-ray diffraction, metallography and EPMA. An α'-Ti (Al,N) solid solution phase rich in Al is found between the nitrided layer and the substrate of Ti-6Al-4V alloy as an obstruction of N_2 to diffuse through the substrate, and then the ionitriding behaviour of the alloy will be alterred. It was also observed that the texture of substrate of these two ionitrided metals varied considerably. Their preferred orientation in inverse-pole-figure of normal sheet changes from (0001) to (o110) and (2131), especially concentrated in the centre part of the specimen. This seems to be the particular phenomenon owing to the ionitriding technique.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/221

1 张立新;李黎光;银耀德;赵齐;张丙申,金属学报,16(1980) ,411.
2 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸,金属学报,17(1981) ,233.
3 姜钟硕;张立新;李黎光;裴秀茹;李铁藩,金属热处理学报,2(1981) ,46.
4 张立新;李黎光,金属学报,18(1982) ,402.
5 傅道斌;严才富;诸乃先;姜进才;孙洪斌,未公开发表材料,1980.
6 Von Bollinger, H., MetaIloberflaeche, 31 (1977) ,329.
7 黄辉;杜树芳,金属热处理,(1980) ,№12,33.
8 彭宏珍,未公开发表资料.
9 张立新;李黎光,金属学报,20(1984) ,B35
10 Pearson, W.B., Lattice Spacings and Structure of Metals and Alloys, Pergamon Press, London, 1958, p. 385, 875.
11 Holmberg, B., Acta Chem. Scand., 16 (1962) , 1255."
No related articles found!
No Suggested Reading articles found!