ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12)
CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 24 May; 1983; revised manuscript 17 November; 1983)
Cite this article: 

CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 24 May; 1983; revised manuscript 17 November; 1983). ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12). Acta Metall Sin, 1984, 20(5): 441-445.

Download:  PDF(363KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The 350℃ isothermal annealing kinetic behaviour and the temperature dependence of the magnetization-and strain-induced magnetic anisotropy constants, K_(um) and K_(us), of the metallic glass Fe_(78)Si_(10)B_(12) have been studied. The K_(um) of positive value varies with annealing time t_a as a linear function of lg t_a and with temperature T in proportion to M_s~(4.6)(T). However, the K_(us) of negative value varies reversibly in a relaxation manner when tension is applied to or removed from the annealed samples and with temperature T in proportion to M_s~(7.5)(T). The behaviour has been qualitatively interpreted using a distortion-directional ordering model.
Received:  18 May 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I5/441

1 陈笃行,金属学报,20(1984) .B212.
2 Gibbs, M. R. J. ; Evetts, J. E. ; Leake, J. A. , Activation Energy Spectra and Relaxation in Amorphous Materials, 1982, (preprint).
3 Egami, T. ; Flanders P. J. , AIP Conf. Proc. , 29 (1976) , 220.
4 Allia, P. ; Soardo, G. P. ; Vinai, F. , Solid State Commun. , 24 (1977) , 517.
5 O'Handley, R. C. , Phys. Rev. , B18 (1978) , 930.
6 Luborsky, F. E. , AIP Conf. Proc. , 29 (1976) , 209.
7 Egami, T. , Amorphous Metallic Alloys, Ed. Luborsky, F. E. , Butterworths, London, 1983 (Preprint).
No related articles found!
No Suggested Reading articles found!