Acta Metall Sin  1984, Vol. 20 Issue (5): 431-440    DOI:
Current Issue | Archive | Adv Search |
INVESTIGATION OF MAGNETIC STABILITY OF CERTAIN Co-BASE AMORPHOUS ALLOYS
CHEN Guojun; ZHANG Wuxin; ZHANG Jiaji (Beijing Metallurgy Research Institute) (Manuscript received 2 September; 1982)
Cite this article: 

CHEN Guojun; ZHANG Wuxin; ZHANG Jiaji (Beijing Metallurgy Research Institute) (Manuscript received 2 September; 1982). INVESTIGATION OF MAGNETIC STABILITY OF CERTAIN Co-BASE AMORPHOUS ALLOYS. Acta Metall Sin, 1984, 20(5): 431-440.

Download:  PDF(726KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of the environmental conditions, such as temperature (—78—100℃), 100℃ aging, vibration, collision, shock and acceleration, on the DC and AC magnetic properties of five types of zero-magnetostrictive Co-base amorphous alloys have been stadied. These five alloys are chosen from that of low loss at high frequency, high initial permeability, square loop, high excursion range of induction and constant permeability respectively. All results were compared with five similar crystalline permalloys. The possible causes of various effects on magnetic properties were analyzed. Their suitability for various uses has also been dicussed.
Received:  18 May 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I5/431

1 Fujimori, H. ; Kikuchi, M. ; Obi, Y. ; Masumoto, T. , Sci. Rep. Rev. Inst. Tohoku Univ. , A26 (1976) , 36.
2 Ohnuma, S.; Masumoto, T. , Rapidly Quenched Metals Ⅲ, Vol. 2, 3rd Int. Conf. , bald at Univ. of Sussex, Brighton, U. K. , July, 1978, Ed. Cantor, B. , The Metals Society, 1978, p. 197.
3 Ohnuma, S. ; Masumoto, T. , J. Appl. Phys. , 50 (1979) , 7597.
4 O'Handley, R. C. ; Narasimhan, M. C. , IEEE Trans. Magn. , MAG-15 (1979) , 970.
5 Luborsky, F. E. , Amorphous Magnetism Ⅱ, Pro. of the 2nd Int. Symp. on Amorphous Magnetism, hald at Rensselaer Polytechnic Inst. , Aug. 1976, Eds. Levy, R. A. ; Hasegawa, R. , Plenum Pr. , New York, 1977, p. 345.
6 Luborsky, F. E. , IEEE Trans. Magn. , MAG-14 (1978) , 1008.
7 Luborsky, F. E. ; Frischmann, P. G. ; Johnson, L. A. , J. Magn. Magn. Mater. , 19 (1980) , 130.
8 Fujimori, H. ; Olta, S. ; Masumoto, T. ; Nakamoto, K. , Rapidly Quenched Metals Ⅲ, Vol. 2, 3rd Int. Conf. , hald at Univ. of Sussex, Brightom U. K. , July, 1978, Ed. Canton, B. , The Metals Soc. , 1978, p. 232.
9 #12
10 #12
11 高橋実;宫崎照宣;渡部明夫,日本金属学会誌,43(1979) ,339.
12 Kohmoto, O. ; Yamaguchi, N; Ohya, K. ; Fujishima, H. , Jpn. J. Appl. Phys. , 17 (1978) , 257
No related articles found!
No Suggested Reading articles found!