Abstract The 350℃ isothermal annealing kinetic behaviour and the temperature dependence of the magnetization-and strain-induced magnetic anisotropy constants, K_(um) and K_(us), of the metallic glass Fe_(78)Si_(10)B_(12) have been studied. The K_(um) of positive value varies with annealing time t_a as a linear function of lg t_a and with temperature T in proportion to M_s~(4.6)(T). However, the K_(us) of negative value varies reversibly in a relaxation manner when tension is applied to or removed from the annealed samples and with temperature T in proportion to M_s~(7.5)(T). The behaviour has been qualitatively interpreted using a distortion-directional ordering model.
|
|
Received: 18 May 1984
|
1 陈笃行,金属学报,20(1984) .B212. 2 Gibbs, M. R. J. ; Evetts, J. E. ; Leake, J. A. , Activation Energy Spectra and Relaxation in Amorphous Materials, 1982, (preprint). 3 Egami, T. ; Flanders P. J. , AIP Conf. Proc. , 29 (1976) , 220. 4 Allia, P. ; Soardo, G. P. ; Vinai, F. , Solid State Commun. , 24 (1977) , 517. 5 O'Handley, R. C. , Phys. Rev. , B18 (1978) , 930. 6 Luborsky, F. E. , AIP Conf. Proc. , 29 (1976) , 209. 7 Egami, T. , Amorphous Metallic Alloys, Ed. Luborsky, F. E. , Butterworths, London, 1983 (Preprint). |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|