CRYSTAL GROWTH OF ARMCO IRON,ELECTROLYTIC IRON AND DILUTE SOLID SOLUTION Fe-Ti ALLOYS
SUN Tizhong;GE Qinglin;CHEN Yuan Shanghai Institute of Metallurgy;Academia Sinica
Cite this article: 

SUN Tizhong;GE Qinglin;CHEN Yuan Shanghai Institute of Metallurgy;Academia Sinica. CRYSTAL GROWTH OF ARMCO IRON,ELECTROLYTIC IRON AND DILUTE SOLID SOLUTION Fe-Ti ALLOYS. Acta Metall Sin, 1985, 21(1): 47-53.

Download:  PDF(1877KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The crystal growth of Armco iron,electrolytic iron and dilute solid solutionalloys,Fe-0.05wt-%Ti and Fe-0.5wt-%Ti,has been investigated by the strain-annealtechnique.The effect of the critical strain and sheet thickness on the grain growthproperties has also been discussed.It was found that the coarse single crystalscould be easily grown up in the cold-rolled Fe-0.28wt-% Ti alloy sheet about 0.1—1mm in thickness only by single high temperature annealing in a wet or dry H_2 atmos-phere without critical strain.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/47

1 Stein,D.F.;Low,J.R.,Jr.,Trans.Metall.Soc.AIME,221(1961) ,744.
2 Irmer,V.;Feller-Kinepmeier,M.,Philos.Mag.,25(1972) ,1345.
3 葛庆麟;施天生;陈廷国;陈源;吴自良;金属学报,18(1982) .316.
4 Bailey,D.J.;Brewer,E.G.,Metall.Trans.,6A(1975) ,403.
5 Hu Hsun;Podgurski,H.H.,Trans.Metall Soc.AIME,233(1965) ,1113.
6 Tomalin,D.S.;McMahon,C.J.,Jr.,Mater.Sci.Eng.,8(1971) ,54.
7 Smallman,R.E.,Modern Physical Metallurgy,Butterworths,London,1962,p.235.
8 Takeuchi,T.,Trans.Jpn Inst.Met.,7(1966) ,1.
No related articles found!
No Suggested Reading articles found!