Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (1): 40-46    DOI:
Current Issue | Archive | Adv Search |
ON THE LONG RANGE ORDER PARAMETERS OF CERTAIN A-15 TYPE COMPOUNDS
ZHANG Hong Shanghai Institute of Metallurgy.Academia Sinica
Cite this article: 

ZHANG Hong Shanghai Institute of Metallurgy.Academia Sinica. ON THE LONG RANGE ORDER PARAMETERS OF CERTAIN A-15 TYPE COMPOUNDS. Acta Metall Sin, 1985, 21(1): 40-46.

Download:  PDF(530KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A review using the structural factor F(S_(6c),y)was carried out for the longrange order parameters of certain A-15 type compounds composed of A_(1-y)B_y cal-culated previously by Van Routh et al.and by Wang et al.from X-ray data.Itwas found that the weight factors in objective functions for analysis and calcu-lation by them seem to be doubtful and the conclusion drawn therefrom aboutthe order-disorder states in these compounds should be reexamined.The criterionwith a minimum error on calculation of the long range order parameters may beproposed by comparison between the composition y from X-ray intensity analysisand y_0 from other accurate determination.Therefore,a neccessary condition maybe suggested for ascertaining the modified weight factors in objective functions,and then the long range order parameters,i.e.,y should be equal to or approxi-mate to y_0.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/40

1 Van Reuth,E.C.;Waterstrat,R.M.,Acta Crystallogr.,B24(1968) ,186.
2 Blaugher,R.E.;Hein,R.E.;Cox,J.E.;Waterstrat,R.M.,J.Low Temp.Phys.,1(1969) ,539.
3 Wang,F.E.;Holden,J.R.,Solid State Commun.,17(1975) ,225.
4 许顺生.金属X射线学,上海科学技术出版社,1962,p.108,182.
5 李惕碚,实验的数学处理,科学出版社,北京,1980,p.265.
6 Waterstrat,R.M.,Solid State Commun.,18(1976) ,531.|
No related articles found!