STRAIN ENERGY PARTITIONING AND ITS APPLICATION TO GH33A Ni-BASE SUPERALLOY AND 1Cr18Ni9Ti STAINLESS STEEL
HE Jinrui;DUAN Zuoxiang;NING Youlian;ZHAO Di Beijing Institute of Aeronautical Materials
Cite this article: 

HE Jinrui;DUAN Zuoxiang;NING Youlian;ZHAO Di Beijing Institute of Aeronautical Materials. STRAIN ENERGY PARTITIONING AND ITS APPLICATION TO GH33A Ni-BASE SUPERALLOY AND 1Cr18Ni9Ti STAINLESS STEEL. Acta Metall Sin, 1985, 21(1): 54-63.

Download:  PDF(815KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The strain energy partitioning(SEP)approach,namely,a modification ofstrain-range partitioning(SRP),has been developed to predict the creep fatiguecrack initiation life for GH33A Ni-base superalloy at 700℃ and 1Cr18Ni9Ti stain-less steel at 600℃.It shows that the life can be predicted by two variables:themaximum tensile stress and the partitioned inelastic strain-range,i.e.,the strain-range component in SRP is substituted by the strain energy component in SEP.The low-cycle fatigue data at elevated temperature for these two given alloys arecorrelated and predicted to within a factor of 2 using SEP,while some numeralsof data for GH33A beyond the factor of 2 using SRP.In addition,the predica-bility of SEP versus SRP has been evaluated by 8 other alloys of high-strengthand low-ductility.It would seem that SEP is an improvement over SRP.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/54

1 Manson,S.S.,Advances in Creep Structures,Eds.Smith,A.I.;Nichlson,A.M.,Applied Science Publishers,London,1971,p.229.
2 Manson,S.S.,Int.J.Fract.Mech.,2(1966) ,№ 1,32.
3 Halford,G.R.;Manson,S.S.,ASM Trans.Q.,61(1968) ,№ 1,94.
4 Berling,J.T.;Coway,J.B.,Metall.Trans.,1(1970) ,600.
5 Snaeb,R.E.;Bui-Quoc,T.,Creep and Fatigue in Elevated-Temperatures Applications,Pro.Int.Conf.,IME-ASME-ASTM,Vol.1,Mechanical Engineering Publishers,London,1973,p.186.
6 Manson,S.S.,NASA TM X-67838,1971,p.1.
7 Coffin,L.F.Jr.,Symp.on Creep-Fatigue Interaction,Ed.Curran,R.M.,Metal Properties Council,New York,1976,p.349.
8 Ostergren,W.J.,ASTM Standardization News,4(1976) ,327.
9 Majumdar,S.;Maiya,P.S.,ANL-76-58,1976,p.1.
10 何晋瑞,未发表资料,1980.
11 宁友连,段作祥,第一届高温疲劳及高温应变测试技术讨论会论文摘要汇编,卷1,中国航空学会理化测试学组,成都,1982,p.148.
12 段作祥;宁友连,ibid.,卷1,1982 p.132.
13 Berstein,H.L.,AFML TR-79-4075,1979.
14 Manson,S.S.,AGARD CP-243,1978.
15 Hyzak,J.M.;Berstein,H.L.,AGARD CP-243,1978,p.5.
16 Halford,G.R.;Nachtigall,A.J.,15th Joint Propulsion Conf.,AIAA/SAE/ASME,1979,U.S.,p.10.