FRACTURE ANALYSIS OF HYDROGEN-INDUCED CRACKING FOR STEEL 12Ni3CrMoV
CHENG Yongxing;ZHOU Peizhi;YU Guanhao Institute No.11 of China State Shipbuilding Corp.Shanghai
Cite this article: 

CHENG Yongxing;ZHOU Peizhi;YU Guanhao Institute No.11 of China State Shipbuilding Corp.Shanghai. FRACTURE ANALYSIS OF HYDROGEN-INDUCED CRACKING FOR STEEL 12Ni3CrMoV. Acta Metall Sin, 1985, 21(1): 75-150.

Download:  PDF(2161KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A fracture analysis on an implant made of steel 12Ni3CrMoV containing 6ppm B was carried out of the dependence of the fracture morphology of hydrogen-induced cracking upon the hydrogen content in HAZ and upon the stress applied.It was shown that its fracture is of the quasi-cleavage(QC)crack of hydrogenembrittlement Its QC region on the fracture surface may be broadened ornarrowed with the increasing of the hydrogen content or the applied stressrespectively.The crystallographic orientation of the QC cracking in HAZ wasverified to be{110}plane by means of the etch-pit method.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/75

1 Kikuta,Y.;Araki,T.;Kuroda,T.,Am.Soc.Test.Mater.,Spec.Tech.Publ.,№ 645,(1980) ,p.107.
2 Beachem,C.D.,Metall.Trans.,3(1972) ,431.
3 Savage,W.F.;Nippes,E.F.;Homma,H.,Weld.J.(New York),55(1976) ,368-s.
4 Savage,W.F.;Nippes,E.F.;Sawhill,Jr.,J.M.,ibid.,55(1976) ,400-s.
5 罗志昌;田燕,李乃迭;闻人琪清华大学学报,21(1981) ,№ 3,35.
6 冶金部钢铁研究总院;北京钢厂;齐齐哈尔钢厂合编,合金钢断口分析金相图谱,科学出版社,北京,1979,p.136.
7 菊田米男;荒木孝雄;黑田敏雄,溶接学会志,44(1975) ,№ 2,168.
8 松田福久;中川博二,走查型电子显微镜汇(?)溶接部破坏面(?)集,黑木出版社,大阪,1979,p.200.
9 贺信莱,硼钢研究文集,冶金部钢铁研究总院主编,冶金工业出版社,1981,p.23.
10 王琰;丁福保;张必强,硼对12Ni3CrMoV钢冷裂敏感性的影响,上海交通大学资料,1980.
11 吴连生,理化检验,物理分册,18(1982) ,№ 2,3.
12 上海交通大学《金属断口分析》编写组,金属断口分析,国防工业出版社,北京,1979,p.11.
13 Kikuta,Y.;Araki,T.,International Institute of Welding,DOC II-927-80,IX-1165-80,(1980) .
No related articles found!
No Suggested Reading articles found!