Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (1): 69-74    DOI:
Current Issue | Archive | Adv Search |
TEMPERATURE DEPENDENCE OF FRACTURE TOUGHNESS OR YIELD STRENGTH OF LOW CARBON STEEL
LONG Qiwei(Lung Chi-wei)Institute of Metal Research;Academia Sinica;Shenyang
Cite this article: 

LONG Qiwei(Lung Chi-wei)Institute of Metal Research;Academia Sinica;Shenyang. TEMPERATURE DEPENDENCE OF FRACTURE TOUGHNESS OR YIELD STRENGTH OF LOW CARBON STEEL. Acta Metall Sin, 1985, 21(1): 69-74.

Download:  PDF(471KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature dependence of fracture toughness of materials seems to haveanalogy to that of yield strength.This similarity for low-carbon steel has beenapproached on the basis of the plastic work loss at the crack tip.Both obey theexponential law and are in agreement with experiment.The availability to enquirefor the temperature dependence of fracture toughness for certain materials otherthan low-carbon steel from that of yield strength has been also discussed.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/69

1 Hahn,G.T.;Hoagland,R.G.;Rosenfield,A.R.,Metall.Trans.,2(1971) ,537.
2 龙期威;何青;周敬,物理学报,21(1965) ,1264.
3 Zwiesele,S.;Diehl,J.,Strength of Metals and Alloys,Proc.of the 5th Int.Conf.Aachen,Federal Republic of Germany,Aug.1979,Eds.Haasen,P.;Gerold,V.;Kostorz,G.,Vol.3,Pergamon Press,1980,p.59.
4 周敬;何青;邹本三;龙期威,科学通报,17(1966) ,497.
5 Petch,N.J.,Philos.Mag.,3(1958) ,1089.
6 #12
7 中村素;内木虎藏;冈林久喜,日本金属学会志,36(1972) ,82.
8 龙期威;高桦,金属学报,19(1983) ,A225.
9 何青;熊良钺;龙期威,科学通报,17(1966) ,500.
10 Hutchison,M.M.,Philos.Mag.,8(1963) ,121.
11 中国科学院金属研究所,东北电力局技术改进局金属室,阜新发电厂金属室,机械工程学报,17(1981) ,62
No related articles found!
No Suggested Reading articles found!