EQUILIBRIUM OF Y-S-O IN LIQUID Ni
WANG Longmei;DU Ting Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing
Cite this article: 

WANG Longmei;DU Ting Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing. EQUILIBRIUM OF Y-S-O IN LIQUID Ni. Acta Metall Sin, 1985, 21(3): 75-82.

Download:  PDF(580KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The deoxysulphurization constant of Y and Y oxysulphide standard free energyof formation vs temperature have been determined in liquid Ni.(?)(?)After calculation by thermodynamic analysis,it was resulted that the equilibriumspace diagram for[Y]-[S]-[O]system and a_O-a_S equilibrium phase diagram in liquidNi are presented.Thus,the subsequence and type of the inclusion formation maybe predicted by them.And the formula controlling the morphology of inclusionformed in liquid Ni by Y addition,as well as the relationship between the Y ad-dition and the content of O_2 and S are also given.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/75

1 Ejima,A.;Suzuki,K.-I.;Harada,N.;Sanbongi,K.,Trans.Iron Steel Inst.Jpn.,17(1977) ,349.
2 Bùzek,Z.,Chemical Metallurgy of Iron and Steel,ISI,London,1973,p.173.
3 Fischer,W.A.;Bertram,H.,Arch.Eisenhuettenwes.,44(1973) ,87.
4 王常珍;王福珍;杜英敏,张小平,金属学报,16(1980) ,1,83.
5 韩其勇;吴卫江;方克明;霍成章;周小龙,中日钢铁学术会议,第一届炼钢学术会议报告,北京,1981,p.25.
6 王龙妹;杜挺,钢铁研究总院学院,3(1983) ,№1,30.
7 Wilson,W.G.,Electr.Furnace conf.Proc.,31(1973) ,p.154.
8 Vahed,A.;Kay,D.A.R.,Metall.Trans.,7B(1974) ,375.
9 Fruehan,R.J.,Metall.Trans.,10B(1979) ,143.
10 McLean,A.H.;Lu,S.K.,Met.Mater.,8(1974) ,№10,452.
11 Fischer,W.A.;Ackermann,W.,Arch.Eisenhuettenwes.,37(1966) ,43.
12 魏寿昆,钢铁,(1980) ,№8,57.
13 王龙妹;杜挺,金属学报,20(1984) ,A287.
14 B(?)zek,Z.,Hutn.Listy,34(1979) ,699.
15 Venal,W.V.;Geiger,G.H.,Metall.Trans.,4(1973) ,2567.
16 王龙妹;杜挺,Ni液中Y-O平衡的研究(待发表).
No related articles found!
No Suggested Reading articles found!