A NEW METHOD FOR CALCULATING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM FROM AN ACTIVITY RATIO FUNCTION OF TWO COMPONENTS
WANG Zhichang Shanghai Institute of Nuclear Research;Academia Sinica
Cite this article: 

WANG Zhichang Shanghai Institute of Nuclear Research;Academia Sinica. A NEW METHOD FOR CALCULATING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM FROM AN ACTIVITY RATIO FUNCTION OF TWO COMPONENTS. Acta Metall Sin, 1985, 21(3): 65-74.

Download:  PDF(543KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Let τ be the function of activity ratio of two components B and C definedby given equation.A new method is proposed which can be used for calculatingthe activities of all the components in a ternary system A-B-C from the knownτ function only by using one set of graphical integration and one set of graphicaldifferentiation.In order to make the calculation with greater accuracy,the discrim-inant which can verify the reliability of integration and differentiation resultsrespectively by using the selected thermodynamic properties of binary systems arealso suggested.The method may also be available to multicomponent systems.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/65

1 周国治,中国科学,(1977) ,№5,456.
2 周国治.中国科学,(1978) ,№3,312.
3 王之昌,金属学报,17(1981) ,168.
4 王之昌;周国治,中国科学,(1984) ,№10,959.
5 徐元森,邹元爔,化学学报,29(1963) ,181.
6 邹元爔,金属学报,6(1963) ,83.
7 邹元爔,中国科学,13(1964) ,1348.
8 彭瑞伍;陈自姚;邹元爔,金属学报,8(1965) ,401.
9 沈令康;韩兆隆;赵彭年;邹元爔,金属学报,9(1966) ,226.
10 邹元爔;周继程;徐元森;赵彭年;张子青,金属学报,18(1982) ,127.
11 周国治,金属学报,8(1965) ,545.
12 Belton,G.R.;Fruehan,R.J.,J.Phys.Chem.,71(1967) ,1403.
13 Kambayashi,S.;Kato,E.,J.Chem.Thermodyn.,15(1983) ,701.
14 徐元森;邹元爔;刘辅链,金属学报,7(1964) ,24.
15 Arita,M.;Pierre,G.R.St.,Trans.Jpn.Inst.Met.,18(1977) ,552.
16 Belton,G.R.;Fruehan,R.J.,Metall.Trans.,2(1971) ,291.
17 Darken,L.S.,J.Am.Chem.Soc.,72(1950) ,2909.
18 周国治;Elliott,J.F.,Proc.,Carl Wagner Symposium,Annual AIME Meeting,Chicago,Illinois'p.195,1981.
19 Elliott,J.F.;Chipman,J.,J.Am.Chem.Soc.,73(1951) ,2682.
20 魏寿昆,活度在冶金物理化学中的应用,中国工业出版社,1964.
21 Moser,Z.;Zabdyr,L.,High Temp.-High Pressures,7(1975) ,425.
22 王之昌,金属学报,18(1982) ,141.
23 Toop,G.W.,Trans.Metall.Soc.AIME,233(1965) ,850.
24 Bertrand,G.L.;Acree,W.E.,Jr.;Burchfield,T.E.,J.Solution Chem.,12(1983) ,327.
25 Hultgren,R.;Desal,P.D.;Hawkins,D.T.;Gleiser,M.;Kelley,K.K.,Selected Values of the Thermodynamic Properties of Binary Alloys,ASM,Metals Park,Ohio,1973,p.400,402,608,610.
No related articles found!
No Suggested Reading articles found!