Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (5): 31-36    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF MINOR Ni OR/AND Cr CONTENTS ON COHERENCE OF OXIDIZED LAYER WITH LOW CARBON STEEL SUBSTRATE
LU Guanfu;GU Jianzhong;WU Guangya Shanghai Iron and Steel Research Institute
Cite this article: 

LU Guanfu;GU Jianzhong;WU Guangya Shanghai Iron and Steel Research Institute. EFFECT OF MINOR Ni OR/AND Cr CONTENTS ON COHERENCE OF OXIDIZED LAYER WITH LOW CARBON STEEL SUBSTRATE. Acta Metall Sin, 1985, 21(5): 31-36.

Download:  PDF(1784KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation was made of the effect of minor Ni or/and Cr additions onthe structure and coherence of the oxidized layer with the low carbon steel substra-te prior to exposure under furnace atmosphere at 1100-1250℃ by means of metal-lography,X-ray diffraction and EPMA.It was observed that at temperature over1150℃,the minor Ni addition improves the coherence of the oxidized layer ofwhich the grain boundary oxidizing structure is formed with Nienriched net-worksand grains wedged into the substrate,while the minor Cr addition has no effecton the structure of the oxidized layer.If the minor Ni and Cr additions coexisted,their coherent layer thickens remarkably.Thus,The addition of minor Ni and Crmay significantly improve the coherence of their oxidized layer on low carbonsteel.
Received:  18 May 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I5/31

1 刘怀文;臧锦,新金属材料,(1974) ,№11,12.
2 Rolls,R.;Arnold,F.V.,Werkst.Korros.,23(1972) ,886.
3 大村泰山;佐平健彰;迫冈晃彦;米泽登,铁(?)钢,62(1976) ,1550.
4 斋藤安俊;桐生坚;木村孝;天野忠昭;矢岛圣使;日本金属学会志,39(1975) ,1110.
5 Kiessling,R.;Lange,N.,钢中非金属夹杂物,第一部分,金属研究所夹杂物研究组译,1973.
6 内山郁,热处理,12(1972) ,145.
No related articles found!
No Suggested Reading articles found!