Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (5): 20-30    DOI:
Current Issue | Archive | Adv Search |
KINETICS OF AUSTENITIZATION DURING INTERCRITICAL ANNEALING OF LOW CARBON LOW ALLOY STEELS
LEI Tingquan;PAN Jie Harbin Institute of Technology
Cite this article: 

LEI Tingquan;PAN Jie Harbin Institute of Technology. KINETICS OF AUSTENITIZATION DURING INTERCRITICAL ANNEALING OF LOW CARBON LOW ALLOY STEELS. Acta Metall Sin, 1985, 21(5): 20-30.

Download:  PDF(2803KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The kinetics of austenitization during intercritical annealing at temperaturesbetween 740 and 820℃ has been studied on the low carbon low alloy steels witha prior microstructure of ferrite-pearlite.In austenitization process,two stages,namely,nucleation and rapid growth of austenite,and slow growth of austeniteinto ferrite are presented.The austenite nucleates mainly along the ferrite-pearliteinterfaces at 740℃,but part of the austenite nuclei forms along the ferrite-ce-mentite boundaries in pearlite colony at 780 and 820℃.The kinetics of the formerstage examined obeys the Cahn's theory of grain boundary nucleation transforma-tion.An attempt is made to discuss the kinetics of the later stage by the theoryof grain growth on recrystallization.
Received:  18 May 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I5/20

1 Speich,G.R.;Demarest,V.A.;Miller,R.L.,Metall.Trans.,12A(1981) ,1419.
2 Speich,G.R.;Miller,R.L.,Ind.Heat.,49(1982) ,25.
3 Garcia,C.I.;DeArdo,A.J.,Metall.Trans.,12A(1981) ,521.
4 Souza,M.M.;Guimaraes,J.R.C.;Chawla,K.K.,Metall.Trans.,13A(1982) ,575.
5 Andrews,K.W.,J.Iron Steel Inst.,203(1965) ,721.
6 Cahn,J.W.,Acta Metall,4(1956) ,449.
7 Cahn,J,W.,Trans.AIME,209(1957) ,140.
8 Cahn,J.W.,Acta Metall.,7(1959) ,18.
9 Speich,G.R.;Szirmae,A.,Trans.Metall.Soc.AIME,245(1969) ,1063.
10 Srolovitz,D.J.;Anderson,M.P.;Grest,G.S.;Sahni,P.S.,Scr.Metall.,17(1983) ,241.
11 Dirnfeld,S.F.;Korevaar,B.M.;Spijker,F.V.,Metall.Trans.,5(1974) .1437
12 Well,C.;Batz,W.;Mehl,R.F.,Trans.AIME,188(1950) ,553.
13 Kirkaldy,J.S.;Smith,P.N.;Sharma,R.C.,Metall.Trans.,4(1973) ,624.
14 #1