THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE |
ZHOU Jihua; GUAN Kezhi (Beijing University of Iron and Steel Technology) |
|
Cite this article:
ZHOU Jihua; GUAN Kezhi (Beijing University of Iron and Steel Technology). THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE. Acta Metall Sin, 1986, 22(1): 123-131.
|
Abstract The flow stress of eight alloy structural steels at high strain rate and high temperature has been studied using a cam plastometry compression machine capable of imparting certain given amount of deformation at a constant strain rate. The tests of the deformation temperature, strain rate and amount of deformation ranged between 850—1150℃, 5—80s~(-1) and 5—69% respectively. The effects of them on the flow stress of the steels were examined. The analysis by non-linear regression and comparison between the mathematical models of flow stress with two types of temperature term were conducted. Thus, a mathematical model of flow stress with great confidence of the eight alloy structural steels is proposed, and its regression coefficient is also recommended.
|
Received: 18 January 1986
|
1 孙一康;孙民生,周纪华,钢铁,14 (1979) .№ 2. 94. 2 #12 3 岡本丰彦,住友金属,12 (1960) ,323. 4 日本鋼鉄協会编,西安重型机械研究所译,轧制理论及其应用,1975,p.125. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|