| CALCULATION OF YIELD STRENGTH OF Nb-V MICROALLOY STEEL CONTROLLED-ROLLED INTO DUAL-PHASE γ+α |
| SUN Fuyu; XU Wenehong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
SUN Fuyu; XU Wenehong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). CALCULATION OF YIELD STRENGTH OF Nb-V MICROALLOY STEEL CONTROLLED-ROLLED INTO DUAL-PHASE γ+α. Acta Metall Sin, 1986, 22(1): 115-152.
|
|
|
Abstract The controlled roiling experiments into the dual-phase γ+a region of the Nb-V microalloy steel have been carried out using a pilot roiling mill. The effect of finishing roiling temperature on the microstructure and mechanical properties of the steel was examined. The yield strength components containing the solid solution strengthening, σ_s, precipitation strengthening, σ_p, dislocation strengthening, σ_d, subgrain strengthening, ck_s l~(-1/2) and grain strengthening, k_yd~(-1/2), were estimated so that a new expression is found as:σ_y=σ_i+σ_s+[σ_p~2+σ_d~2+(ck_s l~(-1/2))~2]~(1/2)+k_yd~(-1/2)The σ_y calculated is in quite agreement with the experimental results.
|
|
Received: 18 January 1986
|
1 徐温崇;孙福玉,金属学报,19 (1983) ,A483. 2 马翔,金属学报,21(1985) ,B222. 3 成田贵一;小山伸二;铁鋼,52 (1966) ;788. 4 Irvine, K.J.; Pickering, F.B.; Gladman, T., J.Iron Steel Inst., 205 (1967) , 161. 5 Tanaka, T.; Tabata, N.; Hatamura, T.; Shiga, C., Micro Alloying 75. Proc. of an International Symposium on High-Strength Low-alloy Steels, Wash., 1975. Sponsored by Union Carbide Corporation Metal Division, etc, New York, Union Carbide Corporation, 1977, p. 107-118. 6 Baker, T, N.; Hot Working And Forming Processes, Ed.Sellars, C.M.; Davies, G. J., The Metals Society, London, 1979, p. 32. 7 Hornbogen, E., Strength of Metals and Alloy, Vol. 2, Proc. of the 5th Int. Conf. on Strength of Metals and Alloys. Aachen, W.Germany, 1979, Eds. Heasen, P.;Gerold, V.; Kostorz. G., p. 1661-1680. 8 Kocks, U.F., Ibid., Vol. 3. 1979, p. 1661-1680. 9 Picketing, F.B.; Gladman, T., Metallurgical developments in carbon steels, Held by the Carbon Steels Committee of the British Iron and Steel Research Association and the Iron and Steel Institute, Harrogate, May 15-16 1963, p. 10. 10 Li, J.C,M., J.Appl. Phys. 33 (1962) , 2958. |