THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE
ZHOU Jihua; GUAN Kezhi (Beijing University of Iron and Steel Technology)
Cite this article: 

ZHOU Jihua; GUAN Kezhi (Beijing University of Iron and Steel Technology). THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE. Acta Metall Sin, 1986, 22(1): 123-131.

Download:  PDF(652KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The flow stress of eight alloy structural steels at high strain rate and high temperature has been studied using a cam plastometry compression machine capable of imparting certain given amount of deformation at a constant strain rate. The tests of the deformation temperature, strain rate and amount of deformation ranged between 850—1150℃, 5—80s~(-1) and 5—69% respectively. The effects of them on the flow stress of the steels were examined. The analysis by non-linear regression and comparison between the mathematical models of flow stress with two types of temperature term were conducted. Thus, a mathematical model of flow stress with great confidence of the eight alloy structural steels is proposed, and its regression coefficient is also recommended.
Received:  18 January 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I1/123

1 孙一康;孙民生,周纪华,钢铁,14 (1979) .№ 2. 94.
2 #12
3 岡本丰彦,住友金属,12 (1960) ,323.
4 日本鋼鉄協会编,西安重型机械研究所译,轧制理论及其应用,1975,p.125.
No related articles found!
No Suggested Reading articles found!