| EQUIVALENCE PRINCIPLE BETWEEN NORMALIZED EULER INDICES AND DIAMETER OF METAL GRAIN |
| LIU Guoquan (Beijing University of Iron and Steel Technology) |
|
Cite this article:
LIU Guoquan (Beijing University of Iron and Steel Technology). EQUIVALENCE PRINCIPLE BETWEEN NORMALIZED EULER INDICES AND DIAMETER OF METAL GRAIN. Acta Metall Sin, 1987, 23(1): 86-88.
|
|
|
Abstract From experimental or theoretical aspect,three Euler indices of a polyhedral grain are equal statistically to the mean caliper diameter of the same grain,when all the values of the foresaid parameters being normalized respectively by their average in the space filling polycrystal to which the grain belongs.It seems that the above principle is independent of the type of the metal concerned,provide that the structures are configured in a way that is consistent with the underlying assumption in the derivation of the principle.
|
|
Received: 18 January 1987
|
1 Desch C.J Inst Met,1919;22:241 2 Williams W M,Smith C S.Trans AIME 1952;194:755 3 Okazaki K,Conrad H.Trans Jpn Inst Met,1972;13:198 4 Rhines F N,Patterson B R.Metall Trans 1982;13A:985 5 Liu G Q(刘国权).Ph.D Dissertation.Univ.of Florida,Gainesville FL,1984 6 DeHoff R T,Liu G Q(刘国权).Metall Trans,1985;16A:2007. 7 Smith C S.In:Metal Interfaces,Cleveland:ASM,1952,65E |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|