THE MEASUREMENT OF DYNAMIC CURVES FOR CuCo_2Be ALLOY HEAT-TREATMENT AND ANALYSIS OF STRENGTHENING PHASE OF ALLOY
LIU Hefa; DAI Xueli; SUN Naizhen; GU Mingyuan (Zhenjiang Ship-building Institute; Jiangsu) (Manuscript received 28 April; 1985; revised manuscript 28 April; 1986)
Cite this article: 

LIU Hefa; DAI Xueli; SUN Naizhen; GU Mingyuan (Zhenjiang Ship-building Institute; Jiangsu) (Manuscript received 28 April; 1985; revised manuscript 28 April; 1986). THE MEASUREMENT OF DYNAMIC CURVES FOR CuCo_2Be ALLOY HEAT-TREATMENT AND ANALYSIS OF STRENGTHENING PHASE OF ALLOY. Acta Metall Sin, 1987, 23(2): 123-128.

Download:  PDF(1336KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A convenient and reliable method for measuring the dynamic curves reflecting the effect of various heat-treatments upon the main properties of age-hardening alloys is described, that can be adopted to serve as a reference for determining the best technological parameters of heat-treatment. The method presented is very simple and effective and it has been guaranteed to meet the desired comprehensive requirements. In the study of strengthening phase, new phase-beryllide (Co_n_1>Cu_n_2· Si_n_3) Be_m in the alloy has been found. The composition of the strengthening phase of CuCo2Be alloy has also been analyzed.
Received:  18 February 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I2/123

1 刘祥主编.铸造合金力学及物理性能.机械工业出版社,1984,329-342
2 上海交通大学编.金属与合金的物理性能.上海交通大学,1980,2-49
3 有色金属及其热处理编写组编.有色金属及其热处理,国防工业出版社,1981,36-66;297-303
4 Wikle K G,铍铜合金的热处理,龚俊杰等译.仪表材料,1975;(6) :43-67
5 重有色金属材料加工手册,冶金工业出版社,1979,208.
6 元素的物理化学性质,王勤和等译,1963,117-125
7 Reinbach R, Baer H G. Z Metallk 1969; 60: 453`
No related articles found!
No Suggested Reading articles found!