| DEFORMATION MARTENSITE IN METASTABLE REGION OF Fe-Mn-Al-Cr SYSTEM |
| TIAN Xing; ZHANG Yansheng (Institute of Metal Research; Academia Sinica; Shengyang) (Manuscript received 10 June; 1985; revised manuscript 17 January; 1986) |
|
Cite this article:
TIAN Xing; ZHANG Yansheng (Institute of Metal Research; Academia Sinica; Shengyang) (Manuscript received 10 June; 1985; revised manuscript 17 January; 1986). DEFORMATION MARTENSITE IN METASTABLE REGION OF Fe-Mn-Al-Cr SYSTEM. Acta Metall Sin, 1987, 23(3): 237-239.
|
|
|
Abstract The deformation a′-martensite in metastable Fe-Mn-Al-Cr alloys with the composition of 15—25wt-%Mn, 0-1.5wt-%Al, 0-0.4wt-%C and 0-1.2wt-%Cr has been studied by means of tensile tests at room temperature and -196℃. The following relationship between the quatity of deformation a′-martensite and the degree of deformation was confirmed: ln[a′/(1 -a′)]=lnA+Klnψ Statistical analysis shows that either lnA or K vary with the composition of alloys linearly at room temperature or-196℃.
|
|
Received: 18 March 1987
|
1 Angel T. J Iron Steel Inst, 1954; 177: 165 2 Ludwigson D C, Berger J A. J Iron Steel Inst, 1965; 207: 63 3 田兴,张彦生,师昌绪.金属学报,1986;22:A 101# |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|