| PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM |
| by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986) |
|
Cite this article:
by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986). PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM. Acta Metall Sin, 1987, 23(4): 382-384.
|
|
|
Abstract The phase diagram of NaF-CaCl_2-LiCl system was studied by X-ray phase analysis. It was found that the NaF forms negative deviation molten salt solution with CaG_2-LiCl system. This result was discussed based on some conclusion obtained from the Monte-Carlo simulation of molten salt mixture.
|
|