AVERAGE INTENSITY OF X-RAY DIFFRACTION SPECTRA OF TEXTURE MATERIALS
by LIN Shuzhi; ZHANG Xizhang (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 2 February; 1986; revised manuscript 3 July; 1986)
Cite this article: 

by LIN Shuzhi; ZHANG Xizhang (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 2 February; 1986; revised manuscript 3 July; 1986). AVERAGE INTENSITY OF X-RAY DIFFRACTION SPECTRA OF TEXTURE MATERIALS. Acta Metall Sin, 1987, 23(4): 379-381.

Download:  PDF(208KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The error of average intensity of X-ray diffraction spectra, in the case of not more enough, from specimen of Fe, Al or Zn having obvious texture was studied. The error of average intensity obtained from measured intensity dividing by polar density factor of the inverse pole figure is so large that it can not be used for quantitative phase analysis. The error of average intensity obtained using oscillation sample holder (the intensity is averaged mechanically over the region from 0 to 60 degree of the pole figure) is improved slightly for Fe or Al, but still large for Zn. The satisfactory result is obtained by means of "the double correction method". The error is 2-5% for Fe or Al, and less than 10% for Zn.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/379

1 Mueller M H, Chernock W P, Beck P A. Trans Metall Soc AIME 1958; 212:39
2 Horta S B, Roberts W T, Wilson D V. Trans Metall Soc. AIME, 1969; 245:2525v
No related articles found!