Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (4): 382-384    DOI:
Current Issue | Archive | Adv Search |
PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM
by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986)
Cite this article: 

by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986). PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM. Acta Metall Sin, 1987, 23(4): 382-384.

Download:  PDF(224KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase diagram of NaF-CaCl_2-LiCl system was studied by X-ray phase analysis. It was found that the NaF forms negative deviation molten salt solution with CaG_2-LiCl system. This result was discussed based on some conclusion obtained from the Monte-Carlo simulation of molten salt mixture.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/382

1 阎立诚,朱鸚鹦,陈念贻.高等学校化学学报,1984;6(5) :755
2 Grube G, Rucel W.JCP Reference Data, 1975; 4(4) : 959
3 #12
4 #12
5 #12
6 #12
7 陈念贻,张桂成,金属学报,1961;7:11
No related articles found!