| MEASUREMENT OF O_2 PRESSURE IN Fe-TiO_2 -FeO·TiO_2 AND Fe-FeO ·TiO_2 -2FeO ·TiO_2 SYSTEMS |
| by XUE Xiangxin; JI Chunlin (Northeast University of Technology; Shenyang)(Manuscript received 19 March; 1986; revised manuscript 18 August; 1986) |
|
Cite this article:
by XUE Xiangxin; JI Chunlin (Northeast University of Technology; Shenyang)(Manuscript received 19 March; 1986; revised manuscript 18 August; 1986). MEASUREMENT OF O_2 PRESSURE IN Fe-TiO_2 -FeO·TiO_2 AND Fe-FeO ·TiO_2 -2FeO ·TiO_2 SYSTEMS. Acta Metall Sin, 1987, 23(5): 492-494.
|
|
|
Abstract Oxygen concentration cells with β-Al_2O_3 solid electrolyte Pt
|
|
Received: 18 May 1987
|
1 Choudhury N S. J Electrochem Soc, 1973; 120: 1663 2 东北工学院冶金物理化学专业编.无机物热力学数据,1976 3 Borowiec K, Rosenqvist T. Scand J Metall, 1981; 10: 217 4 Taylor R W, Schmalzried H. J Phys Chem, 1964; 68 (9) : 2444 5 小野腾敏,森山徐一郎.日本鉱业会志,1973;89(1023) :313 6 #12 7 Grey I E, Reid A F, Jones D G. Inst Min Metall Trans, Sect C: Min Process Extr Metall, 1974; 83 (2) : C10 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|