Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 492-494    DOI:
Current Issue | Archive | Adv Search |
MEASUREMENT OF O_2 PRESSURE IN Fe-TiO_2 -FeO·TiO_2 AND Fe-FeO ·TiO_2 -2FeO ·TiO_2 SYSTEMS
by XUE Xiangxin; JI Chunlin (Northeast University of Technology; Shenyang)(Manuscript received 19 March; 1986; revised manuscript 18 August; 1986)
Cite this article: 

by XUE Xiangxin; JI Chunlin (Northeast University of Technology; Shenyang)(Manuscript received 19 March; 1986; revised manuscript 18 August; 1986). MEASUREMENT OF O_2 PRESSURE IN Fe-TiO_2 -FeO·TiO_2 AND Fe-FeO ·TiO_2 -2FeO ·TiO_2 SYSTEMS. Acta Metall Sin, 1987, 23(5): 492-494.

Download:  PDF(228KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Oxygen concentration cells with β-Al_2O_3 solid electrolyte Pt
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/492

1 Choudhury N S. J Electrochem Soc, 1973; 120: 1663
2 东北工学院冶金物理化学专业编.无机物热力学数据,1976
3 Borowiec K, Rosenqvist T. Scand J Metall, 1981; 10: 217
4 Taylor R W, Schmalzried H. J Phys Chem, 1964; 68 (9) : 2444
5 小野腾敏,森山徐一郎.日本鉱业会志,1973;89(1023) :313
6 #12
7 Grey I E, Reid A F, Jones D G. Inst Min Metall Trans, Sect C: Min Process Extr Metall, 1974; 83 (2) : C10
No related articles found!
No Suggested Reading articles found!