| QUENCHING RATE MEASUREMENT FOR AMORPHOUS ALLOY FORMATION |
| by PANG Dexing; WANG Jingtang; LIN Xuerong; SONG Qihong; XU Jun (Institute of Metal Research; Academia Siniea; Shenyang) (Manuscript received 20 July; 1987) |
|
Cite this article:
by PANG Dexing; WANG Jingtang; LIN Xuerong; SONG Qihong; XU Jun (Institute of Metal Research; Academia Siniea; Shenyang) (Manuscript received 20 July; 1987). QUENCHING RATE MEASUREMENT FOR AMORPHOUS ALLOY FORMATION. Acta Metall Sin, 1987, 23(6): 592-593.
|
|
|
Abstract The direct measurement of quenching rate during the amorphous ribbon formation of alloys Fe-Si-B and Ni-P by using an infrared thermal photography technique is described. Experimental results show that the critical quenching rate of amorphous alloy Fe-Si-B or Ni-P formation is 5.0×10~5 or 1.0×10~5℃/s related to the linear wheel speed 17.0 or 12.0 m/s respectively.
|
|
Received: 18 June 1987
|
1 Greer A L. J Mater Sci, 1982; 17: 1117 2 Kattamis T Z, Brower W E, Mehrabian R. J Cryst Growth, 1973; 19: 229 3 Gillen A G, Cantor B. Acta Metall, 1985; 33: 1813 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|