INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH
LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing
Cite this article: 

LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing. INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH. Acta Metall Sin, 1988, 24(1): 82-86.

Download:  PDF(350KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solute distribution in the initial transient during unidirectionalplanar crystal growth has been studied. An expression of solute distributionin liquid phase near liquid-solid interface at the initial growth stage was derived.A method for reducing the length of initial transient was put forward and theshortest initial transient length was determined. The growth velocity function re-quired for realizing the shortest transient length at the initial stage was then ob-tained.
Key words:  crystal growth      solute distribution      composition transient     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/82

1 Tiller W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428
2 闵乃本.晶体生长的物理基础,上海科学技术出版社,1982:58
3 Pohl R G. J Appl Phys, 1954; 23: 1170
4 Flemings M C. Solidification Processing, New York: McGraw-Hill, 1974: 4
[1] CHANG Guowei JIN Guangcan CHEN Shuying LI Qingchun YUE Xudong. STUDY ON LATERAL GROWTH RATE OF PERITECTIC REACTION PRODUCTS[J]. 金属学报, 2011, 47(3): 380-384.
[2] MIN Zhixian SHEN Jun WANG Lingshui FENG Zhourong LIU Lin FU Hengzhi. MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH[J]. 金属学报, 2010, 46(9): 1075-1080.
[3] WANG Qiang MA Mingzhen ZHANG Xinyu LIU Riping. CRYSTAL GROWTH VELOCITY IN UNDERCOOLED Zr50Cu50 ALLOY MELT[J]. 金属学报, 2008, 44(12): 1415-1418.
[4] MA Tianyu; YAN Mi; WANG Qingwei. Homogeneity of Magnetostriction of Tb--Dy--Fe—Co<110> Oriented Alloy Rod[J]. 金属学报, 2007, 43(7): 688-692 .
[5] LI Tao; CHEN Guang; LIN Xin; HUANG Weidong. MORPHOLOGICAL EVOLUTION OFSOLIDIFICATION MICROSTRUCTURE OF BINARY ALLOY UNDER STIRRING[J]. 金属学报, 2006, 42(6): 577-583 .
[6] JIANG Chengbao; LIU Jinghua; ZHANG Tao; XU Huibin. The Solid-Liquid Interface Morphology of the Unidirectionally Solidified Ni2MnGa Magnetic Shape Memory Alloy[J]. 金属学报, 2004, 40(9): 975-980 .
[7] CHEN Changle;LU Fuyi (Northwestern Polytechnical University; Xi'an 710072). STOCHASTIC DYNAMICS FOR NONEQUILIBRIUM SOLUTE DISTRIBUTION AT SOLID-LIQUID INTERFACE[J]. 金属学报, 1997, 33(5): 455-460.
[8] FU Hengzhi; HE Guo; LI Jianguo (State Key Laboratory of Solidification Processing;Northwestern Polytechnical University; Xi'an 710072). OBSERVATION OF COMPETITIVE GROWTH IN A DIRECTIONALLY SOLIDIFIED NICKEL BASE SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 1997, 33(12): 1233-1238.
[9] SHEN Ningfu; TANG Yali; GUAN Shaokang; ZHANG Dongjie (Zhengzhou Institute of Technology; Zhengzhou 450002)(Manuscript received 1995-12-28). SOLIDIFICATION THEORY AND RAPID SOLIDIFICATION[J]. 金属学报, 1996, 32(7): 673-684.
[10] LIU Juncheng; JIE Wanqi; ZHOU Yaohe (State Key Laboratory of Solidificatton Processing; Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 1995-06- 1 9). EXPERIMENTAL STUDY OF THE ACRT EKMAN FLOW[J]. 金属学报, 1996, 32(3): 269-273.
[11] CHANG Fenglian;WANG Shidong; ZHANG Jinping; MEl Jianping;SU Huaqin;(Southeast University;Nanjng 210018)(Manuscript received 94-05-06; in revised form 94-10-18). FORMATION OF SECOND PHASE IN Cu-Zn-Al-Mn-Ni-Ti SMA[J]. 金属学报, 1995, 31(1): 14-18.
[12] WU Qiang;LIU Chi Nanjing University of Science and Technology Southeast University. COMPARISON OF SOLUTE DISTRIBUTION BETWEEN SPHERICAL GROWTH AND DIRECTIONAL SOLIDIFICATION[J]. 金属学报, 1993, 29(9): 42-46.
[13] LU Ke;WANG Jingtang National Laboratory of RSA; Institute of Metal Research; Academia Sinica; Shenyang. A MATHEMATICAL EXPRESSION OF CRYSTAL GROWTTH RATE DURING CRYSTALLIZATION OF AMORPHOUS ALLOYS[J]. 金属学报, 1991, 27(4): 105-110.
[14] LU Ke;WANG Jingtang National Laboratory for RSA; Institute of Metal Research; Academia Sinica. Shenyang; DONG Lin Liaoning Provincial Centre of Analysis and Testing Research. Shenyang. IN SITU OBSERVATION ON DYNAMIC CRYSTALLIZATION IN AMORPHOUS Ni-P ALLOY FOIL[J]. 金属学报, 1991, 27(1): 108-114.
[15] LIU Lin;FU Hengzhi;SHI Zhengxing Northwestern Polytechnical University; Xi'an. RELATIONSHIP BETWEEN PRIMARY MORPHOLOGY AND CRYSTAL STRUCTURE OF MC CARBIDES PRECIPITATED IN SUPERALLOYS[J]. 金属学报, 1989, 25(4): 48-53.
No Suggested Reading articles found!