DENSITY SURFACE TENSION WETTABILITY AND ADHESIVE POWER OF LIQUID Al AND Al-RE ALLOY ON BN SURFACE
BIAN Maoshu Associate Professor;Institute of Metal Research;Academia Sinica;Shenyang;CHEN Qiu;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

BIAN Maoshu Associate Professor;Institute of Metal Research;Academia Sinica;Shenyang;CHEN Qiu;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang. DENSITY SURFACE TENSION WETTABILITY AND ADHESIVE POWER OF LIQUID Al AND Al-RE ALLOY ON BN SURFACE. Acta Metall Sin, 1988, 24(2): 207-209.

Download:  PDF(248KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The density, surface tension, wettability and adhesive power of liquid high purityAl (99.999 wt-%), technical pure Al (99.6 wt-%) and Al-RE alloy on BN plate were measuredusing sessile drop method. The results show that both the density and surface tension graduallydecrease but the adhesive power and wettability gradually increase with increasing temperature.The density increases and the shaface tension, wettability as well as adhesive power decreasewith the increase of RE content respectively.
Key words:  liquid Al and Al-RE alloy      density      surface tension      wellability      adhesive power     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/207

1 储国良.稀土进展,1984;(1) :7
2 Goumiri L, Joud J C, Desre P, Hicter J M. Surf Sci. 1979; 83(2) : 471--486
3 王景唐,边茂恕,曾孟仓.金属学报,1981;17:259
4 王景唐,陈秋,于永田,李谷松.全国第五届冶金过程物理化学年会论文集(上册),1984:335
5 马禄铭,边茂恕,王景唐.全国第五届冶金过程物理化学年会论文集(上册),1984:422
6 Mcevoy A J, Williams R H, Higginbotham I G. J Mater Sci, 1976; 11(2) : 297--302
7 Champion J A, Keene B J, Sillwood J M. J Mater Sci. 1969; 4(1) : 39--49
8 Allen B C. In: Beer S Z ed., Liquid Metals, New York: Dekker, 1972; 186A
[1] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[2] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[3] MA Jiankai, LI Junjie, WANG Zhijun, WANG Yujian, WANG Jincheng. Bonding Zone Microstructure and Mechanical Properties of Forging-Additive Hybrid Manufactured Ti-6Al-4V Alloy[J]. 金属学报, 2021, 57(10): 1246-1257.
[4] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[5] Xingpin CHEN,Wenjia LI,Ping REN,Wenquan CAO,Qing LIU. Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels[J]. 金属学报, 2019, 55(8): 951-957.
[6] Yubi GAO, Yutian DING, Jianjun CHEN, Jiayu XU, Yuanjun MA, Dong ZHANG. Evolution of Microstructure and Texture During Cold Deformation of Hot-Extruded GH3625 Alloy[J]. 金属学报, 2019, 55(4): 547-554.
[7] Qingdong XU, Kejian LI, Zhipeng CAI, Yao WU. Effect of Pulsed Magnetic Field on the Microstructure of TC4 Titanium Alloy and Its Mechanism[J]. 金属学报, 2019, 55(4): 489-495.
[8] Zixing WANG,Shuo HUANG,Beijiang ZHANG,Lei WANG,Guangpu ZHAO. Study on Freckle of a High-Alloyed GH4065 Nickel Base Wrought Superalloy[J]. 金属学报, 2019, 55(3): 417-426.
[9] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[10] Ming HE, Xianliang LI, Qingwei WANG, Lianyu WANG, Qiang WANG. Influence of Magnetic Shielding on the Power Loss of Induction Heating Power Supply in the Electro-magnetic Induction Controlled Automated Steel Teeming System[J]. 金属学报, 2019, 55(2): 249-257.
[11] XIONG Jian,WEI Dean,LU Songjiang,KAN Qianhua,KANG Guozheng,ZHANG Xu. A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient[J]. 金属学报, 2019, 55(11): 1477-1486.
[12] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[13] Runzhi QIN, Yanxia DU, Minxu LU, Li OU, Haiming SUN. Study of Interference Parameters Variation Regularity and Corrosion Behavior of X80 Steel in Guangdong Soil Under High Voltage Direct Current Interference[J]. 金属学报, 2018, 54(6): 886-894.
[14] Jin WANG, Liming YU, Yuan HUANG, Huijun LI, Yongchang LIU. Effect of Crystal Orientation and He Density on Crack Propagation Behavior of bcc-Fe[J]. 金属学报, 2018, 54(1): 47-54.
[15] Yao WANG,Chunfu LI,Yuanhua LIN. Electronic Theoretical Study of the Influence of Cr on Corrosion Resistance of Fe-Cr Alloy[J]. 金属学报, 2017, 53(5): 622-630.
No Suggested Reading articles found!