STUDY OF A NEW TYPE SEMI-LINING ELECTRO-SLAG REMELTING
CHEN Chongxi;GAO Rongfu Beijing University of Iron and Steel TechnologyDeft.of Superalloy;Beijing University of Iron and Steel Technology; Beijing
Cite this article: 

CHEN Chongxi;GAO Rongfu Beijing University of Iron and Steel TechnologyDeft.of Superalloy;Beijing University of Iron and Steel Technology; Beijing. STUDY OF A NEW TYPE SEMI-LINING ELECTRO-SLAG REMELTING. Acta Metall Sin, 1988, 24(3): 221-228.

Download:  PDF(1525KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new type of electroslag refining technique has been proposed andthe influence of superimposed DC density on the contents of active metal elementsas well as on the desulphurization and degassing have been studied. The resultsshow that the enerey consumption may be reduced by 41% by using this technique.During the semi-lining ESR under normal atmosphere, there is no evident loss ofactive metal elements, while the contents of O, N and S can be effectively reducedto 10ppm in superalloys GH49 and GH37. The ingot solidified along its axis andhas a compact microstructure. The secondary dendrite arm spacing of the semiliningESR ingot is about 1/3 shorter than that of tbe general ESR ingot.
Key words:  semi-lining electroslag furnace      electroslag remelting     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/221

1 Elienne M, Mitchell A. Oxidation Losses of Low Levels of titanium During Electroslag Remelting, In: Bhat G K ed. Proc of the Second Int Symp on Electroslag Remelting Technology, Part II, Pittsburgh: Mellon Institute, 1969
2 Knights C F, Perkins R. Electroslag Refining, In: Proc of a Conf on Electroslag Refining, London: Iron and Steel Institute, 1973: 35
3 Gill L L, Harris K. Electroslag Refining, In: Proc of a Conf on Electroslag Refining, London: Iron and Steel Institute. 1973: 89
4 陈崇禧,王涌,傅杰,陈恩普.金属学报,1981;17:50
5 陈崇禧,高荣富,赵文祥.金属学报,1984;20:B137
6 Luchok J, Roberts R J. In: Proc of the 4th Int Symp on Electroslag Remelting Processes, Tokyo: The Iron and Steel Institute of Japan, 1973: 149
7 Holzgruber W. In: Bhat G K, Simkovich A eds. Proc of the 5th Int Symp on Electroslag and Other Special Melting Technologies, Pittsburgh: Carnegie-Meooln Institute, 1974: 70
8 Sullivan C P, Giamei A F, Versnyder F L. In: Bhat G K. Simkovich A eds. Proc of the 5th Int Symp on Electroslag and Other Special Melting Technologies. Pittsburgh: Carnegie-Mellon Institute. 1974: 525
9 #12
10 Holzgruber W, Machner P. Ploeckinger E, Boehler G. In: Foster E L ed. Transaction Vacuum Metallurgy Conf 1969, New York: American Vacuum Society, 1969: 415
11 Cordy J T, Kelley S L, Lherbier L W. In: Bhat G K, Lherbier L W eds. Proc Vacuum Metallutgy Conf 1984, Pittsburgh: Iron and Steel Society, 1984: 69
12 Boehler G, GB Pat 1230183, 1971
[1] Qing LI,Zixing WANG,Shuyuan XIE. Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. 金属学报, 2017, 53(4): 494-504.
[2] NI Zifei SUN Yangshan XUE Feng BAI Jing. STUDY ON FABRICATION, MICROSTRUCTURE AND PROPERTIES OF IN SITU TiC PARTICLE ON DISPERSION–STRENGTHENED 304 STAINLESS STEEL[J]. 金属学报, 2010, 46(8): 935-940.
[3] WANG Fang LI Baokuan. ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES[J]. 金属学报, 2010, 46(7): 794-799.
[4] CHU Shaojun; LIU Haihong; ZHANG Heyi (Metallurgical Engineering College;University of Science and Technology Beijing; Beijing 100083)Correspondent: CHU Shaojun; associate professor; Tel: (010)62332790; Fax: (010)62522845. GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON[J]. 金属学报, 1998, 34(9): 971-976.
[5] WEI Jihe(Shanghai University; 200072); REN Yongli; (Xi'an Institute of Metallurgy and Construction Engineering; 710055)(Manuscript received 94-04-27). MATHEMATICAL SIMULATION OF MAGNETIC FIELD IN ESR SYSTEM[J]. 金属学报, 1995, 31(14): 51-60.
[6] WEI Jihe(WEI Chiho)(Shanghai University);REN Yongli(Xi'an Institute of Metallurgy and Construction Engineering)(Manuscript received 19 February; 1994). MATHEMATICAL MODELLING OF SLAG FLOW FIELD IN ESR SYSTEM[J]. 金属学报, 1994, 30(23): 481-490.
[7] WEI Jihe (Shanghai Univereity.of Technology);LIU Zongyuan(Xi'van Institute of Metallurgy Construction Engineering). STUDY ON OXYGEN TRANSFER THROUGH MOLTEN SLAGS OF CaF_2+Al_2O_3 AND CaF_2+Al_2O_3+CaO SYSTEMS FOR ESR[J]. 金属学报, 1994, 30(20): 350-360.
No Suggested Reading articles found!