| MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS |
| GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang |
|
Cite this article:
GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang. MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS. Acta Metall Sin, 1988, 24(3): 296-298.
|
|
|
Abstract In the amorphous alloys (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x, the magnetic moment and the curietemperature were found to increase slowly with increasing boron and relatively decreasing silicon.This phenomenon has been explained qualitatively in terms of the electron transition model andthe molecular field approtimation theory.
|
|
Received: 18 March 1988
|
1 Ward K D, Crangle J, Davies H A. In: Masumoto T et al. eds. The Magnetic Moments on Fe, Co and Ni Atoms in Amorphous Alloys Containing Boron, Proc 4th Int Conf on Rapidly Quenched Metal, Sendai. Aug 24--28, 1981, Japan: The Japan Institute of Metals, 1982: 1141--1144 2 Kaneyoshi T. In: Hasegawa R ed., Magnetic Chemical and Structural Properties in Glass Metallic Alloys, Cleveland, Ohio: Chemical Rubber Co., 1981: 38--409 |
| No Suggested Reading articles found! |
|
|