FORMATION OF PRECIPITATED AUSTENITE IN 9% Ni STEEL AND ITS FUNCTION AT CRYOGENIC TEMPERATURE
LEI Ming;GUO Yunyi Institute of Metal Research; Academic Sinica; Shenyang
Cite this article: 

LEI Ming;GUO Yunyi Institute of Metal Research; Academic Sinica; Shenyang. FORMATION OF PRECIPITATED AUSTENITE IN 9% Ni STEEL AND ITS FUNCTION AT CRYOGENIC TEMPERATURE. Acta Metall Sin, 1989, 25(1): 13-17.

Download:  PDF(1440KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Streaks of austenite-rich and ferrite-rich bands produce during thesoaking at α+γ region because of the re-distribution of elements. Part of the aus-tenite formed at intermediate temperatures transforms into martensite while thesteel was cooled down to room temperature. The structure which consists of finemartensite and austenite exhibits a moderate strength and high enough cryogenictoughness. One of the important cause of the excellent cryogenic properties is thatthe precipitated austenite absorbs the impurities and thus purifies the matrix of thesteel.
Key words:  9%Ni steel      precipitated austenite      cryogenic toughness     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/13

1 张弗天,许义奎.能源材料通讯,1984;2(4) :58
2 张弗天、王景韫,郭蕴宜.金属学报,1984;20:A405
3 雷鸣.中国科学院金属研究所硕士论文,1985
4 宋建先,中国科学院金属研究所硕士论文,1983S
[1] Meng WANG, Zhenyu LIU, Chenggang LI. Effects of Ultra-Fast Cooling After Hot Rolling and Lamellarizing on Microstructure and Cryogenic Toughness of 5%Ni Steel[J]. 金属学报, 2017, 53(8): 947-956.
[2] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[3] YANG Yuehui CAI Qingwu WU Huibin WANG Hua. FORMATION OF REVERSED AUSTENITE AND ITS EFFECT ON CRYOGENIC TOUGHNESS OF 9Ni STEEL DURING TWO--PHASE REGION HEAT TREATMENT[J]. 金属学报, 2009, 45(3): 270-274.
[4] MENG Xiangmin; LI Guanglai; ZHANG Futian; WU Yakun(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang110015)Comspondent: MENG Xiangmin; Tel: (024)3843531-55491; Fax: (024)3891320; E-mail: lais imr ac.cn. TEM STUDIES OF GRAIN BOUNDARY BETWEEN MARTENSITE LATHES IN 9Ni STEEL[J]. 金属学报, 1998, 34(6): 565-570.
[5] MENG Xiangmin; LI Guanglai; ZHANG Futian; WU Yukun (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Scicnces;Shenyang 110015)(Manuscript received 1995-12-14). LOW-ANGLE TILT GRAIN BOUNDARY BETWEEN MARTENSITE LATHES IN 9Ni STEEL[J]. 金属学报, 1996, 32(7): 700-704.
No Suggested Reading articles found!