FATIGUE CRACK PROPAGATION FOR BIAXIAL STRESS CYCLING
PEI Hongxun Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang
Cite this article: 

PEI Hongxun Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. FATIGUE CRACK PROPAGATION FOR BIAXIAL STRESS CYCLING. Acta Metall Sin, 1989, 25(1): 53-61.

Download:  PDF(604KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the experimental study of complex biaxial mode I fatiguecrack growth and the discussion on Von Mises theory, a new approach is pro-posed for correlating crack propagation rate under both in-phase and out-of-phasebiaxial stress cycling. The results emphasize the contribution of plasticity to fatiguecrack growth.
Key words:  Biaxial stress      fatigue crack growth      nonproportional loading      strain energy density     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/53

1 Brown M W, Miller K J. ASTM STP 770, 1982
2 Garud Y S. J Test Eval, 1981; 9: 165--178
3 Kanazawa K, Miller K J, Brown M W. Trans ASME, Ser. H: J Eng Mater Technol, 1977; 99: 222--228
4 Jordan E H, Brown M W, Miller K J. ASTM STP 853, 1985
5 蔡其巩,金属学报,1977;13:246--262
6 Dowling N E. Trans ASME, Ser. H: J Eng Mater Technol, 1978; 100: 157--163
7 Brown M W, De Los Rios E R, Miller K J. ASTM Symposium on Fundamental Questions and Critical Experiments in Fatigue, Dallas, Texas, USA, 1984
8 Liebowitz H, Lee J D, Eftis J. Eng Fract Mech, 1978; 10: 315--335
9 Starkey M S, Skelton R P. Fatigue Eng Mater Struct, 1982; 5: 329--340
10 Dowling N E. ASTM STP 635, 1977: 97--121
11 Brown M W, Miller K J. ASTM STP 853, 1985
12 Garud Y S. Trans ASME, Ser. H: J Eng Mater Technol, 1981; 103: 118--125*
[1] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[2] Chao XU, Qiliang NAI, Zhihao YAO, He JIANG, Jianxin DONG. Grain Boundary Oxidation Effect of GH4738 Superalloy on Fatigue Crack Growth[J]. 金属学报, 2017, 53(11): 1453-1460.
[3] Qiliang NAI,Jianxin DONG,Maicang ZHANG,Zhihao YAO. INFLUENCE OF MULTI-MICROSTRUCTURE INTERACTION ON FATIGUE CRACK GROWTH RATE OF GH4738 ALLOY[J]. 金属学报, 2016, 52(2): 151-160.
[4] YANG Jian, DONG Jianxin, ZHANG Maicang. HIGH TEMPERATURE FATIGUE CRACK GROWTH BEHAVIOR OF A NOVEL POWDER METALLURGY SUPERALLOY FGH98[J]. 金属学报, 2013, 49(1): 71-80.
[5] LI Wei CHEN Zhenhua CHEN Ding TENG Jie. GROWTH BEHAVIOR OF FATIGUE CRACK IN SPRAY-FORMED SiCp/Al-7Si COMPOSITE[J]. 金属学报, 2011, 47(1): 102-108.
[6] XIONG Ying CHEN Bingbing ZHENG Sanlong GAO Zengliang. STUDY ON FATIGUE CRACK GROWTH BEHAVIOR OF 16MnR STEEL UNDER DIFFERENT CONDITIONS[J]. 金属学报, 2009, 45(7): 849-855.
[7] MO Defeng HE Guoqiu ZHU Zhengyu LIU Xiaoshan ZHANG Weihua. FATIGUE FEATURES AND MECHANISM OF Al--7Si--0.3Mg CAST ALLOY UNDER NONPROPORTIONAL LOADINGS[J]. 金属学报, 2009, 45(7): 861-865.
[8] LU Liantao LI Wei ZHANG Jiwang SHIOZAWA Kazuaki ZHANG Weihua. ANALYSIS OF ROTARY BENDING GIGACYCLE FATIGUE PROPERTIES OF BEARING STEEL GCr15[J]. 金属学报, 2009, 45(1): 73-78.
[9] . The turning point in Paris region of fatigue crack growth in titanium alloy[J]. 金属学报, 2008, 44(8): 973-978 .
[10] XIONG Ying. A TWO-PARAMETER DRIVING FORCE FOR FATIGUE CRACK GROWTH[J]. 金属学报, 2008, 44(11): 1348-1353 .
[11] YU Huichen; ZHANG Yanji; SUN Yanguo; XIE Shishu; TANAKA Keisuke. Near Threshold Fatigue Crack Growth Behavior in Stainless Steel[J]. 金属学报, 2005, 41(7): 721-726 .
[12] YANG Xianjie; GAO Qing; CAI Lixun; LIU Yujie. An Experimental Study on the Deformation Behavior of SS304 Stainless Steel UnderNonproportional Cyclic Stress and Strain at Room Temperature[J]. 金属学报, 2004, 40(9): 935-942 .
[13] QIN Ming; JI Vincent JI Ning; LI Jiabao; MA Suyuan; CHEN Changrong; SONG Zhongxiao; HE Jiawen. RELATIONSHIP BETWEEN THE YIELD STRENGTH AND ANNEALING TEMPERATURE OF A Cu FILM ADHERENT TO SUBSTRATE[J]. 金属学报, 2004, 40(7): 716-720 .
[14] XIAO Lin(State Key Laboratory for Mechanical Behaviour of Materials; Xi'an Jiaotong University; Xi'an 710049)KUANG Zhenbang(Department of Engineering Mechanics; Shanghai Jiaotong University; Shanghai 200030). MACROSCOPIC RESPONSE AND MICROSCOPIC MECHANISM OF ZIRCALOY-4 UNDER NONPROPORTIONAL LOADING[J]. 金属学报, 1998, 34(3): 242-248.
[15] CHEN Wenzhe;ZHANG Sa;QIAN Kuangwu (Department of Materials; Fuzhou University; Fuzhou 350002)GU Haicheng (Institute of Materials; Xi'an Jiaotong University; Xi'an 710049)WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). FATIGUE CRACK GROWTH RATES AND FATIGUE THRESHOLDS OF CENTRIFUGAL SPRAY DEPOSITED Ti-48Al-2Mn-2Nb[J]. 金属学报, 1998, 34(1): 70-74.
No Suggested Reading articles found!