| SURFACE ANALYSES OF NITROGEN ION IMPLANTED Ti6A14V ALLOY |
| ZHAO Guozhen;YU Jian;ZHANG Xiaozhong Shanghai Research Institute of Materials Tsinghua University |
|
Cite this article:
ZHAO Guozhen;YU Jian;ZHANG Xiaozhong Shanghai Research Institute of Materials Tsinghua University. SURFACE ANALYSES OF NITROGEN ION IMPLANTED Ti6A14V ALLOY. Acta Metall Sin, 1989, 25(3): 119-124.
|
|
|
Abstract The techniques for surface analysis including AES, XPS and SIMS wereemployed to study the chemical composition and bond valence of nitrogen ion im-planted surface of surgical implantation service alloy Ti6A14V. The depth of implant-ed nitrogen ions and the sputtering rate of argon beams were determined using pro-filometer. It was found that the combination of injected nitrogen ions with titaniumresulted in the formation of hard TiN particles and the profile of nitrogen concentra-tion approximately displayed gaussian distribution. The total depth of implantednitrogen is about 350nm and its maximum concentration appers in the depth ofabout 140nm from the surface, in which the concentration ratio of nitrogen to tita-nium may be up to 1.1.
|
|
Received: 18 March 1989
|
1 Webb J F. Longer Life Replacement Hip Joints in Prospect, London: London-Press Service, 1984 2 张效忠,张剑强,郭兴唐。全国第三届人工关节学术论文摘要汇编,北京:1986:30 3 赵国珍,华惠中,李丽霞,杨武.理化检验(物理分册),1987;23(1) :10 4 Wagner C D, Riggs W M. Davis L E, Moulder J F, Muilenberg G E. Handbook of X-Ray Photoelectron Spectroscopy, Minnesota: Perkin-Elmer Corporation Physical Electronics Division, 1979 5 Davis L E, Macdonald N C, Palmberg P W, Riach G E, Weber R E. Handbook of Auger Electron Spectroscopy. Minnesota: Physical Electronics Industries, 1978 6 陆家和,陈长彦,曹立礼,薛增泉,查良镇,何炜.表面分析技术,北京:电子工业出版社,1987:174 7 桥本功二,浅见胜彦。防食技术,1977;26:375 8 张光华,钟士谦。离子注入技术,北京:机械工业出版社,198 |
| No Suggested Reading articles found! |
|
|