Abstract The relationship between partition ratio at solid-liquid interface andtemperature gradient or external force field has been theoretically analysed. It isshown that under the action of temperature gradient or external force field, the partitionratio at solid--liquid interface will deviate from the equilibrium value.
|
|
Received: 18 March 1989
|
1 Wood R F. Phys Rev B, 1982; 25: 2786 2 Jackson K A, Gilmer G H, Leamy H J. In: White C W, Peercy P S eds., Laser and Electron Beam Processing of Materials, New York: Academic, 1980: 104 3 Aziz M J. J Appl Phys. 1982; 53: 1158 4 李如生,非平衡态热力学和耗散结构,北京:清华大学出版社,1986:105 5 下地光雄著,郭淦钦译,液态金属,科学出版社,1987:275 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|