PARTITION RATIO AT SOLID-LIQUID INTERFACE UNDER ACTION OF TEMPERATURE GRADIENT AND EXTERNAL FORCE FIELD
GUO Junqing;GU Genda;LI Qingchun Harbin Institute of Technology
Cite this article: 

GUO Junqing;GU Genda;LI Qingchun Harbin Institute of Technology. PARTITION RATIO AT SOLID-LIQUID INTERFACE UNDER ACTION OF TEMPERATURE GRADIENT AND EXTERNAL FORCE FIELD. Acta Metall Sin, 1989, 25(3): 130-133.

Download:  PDF(275KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The relationship between partition ratio at solid-liquid interface andtemperature gradient or external force field has been theoretically analysed. It isshown that under the action of temperature gradient or external force field, the partitionratio at solid--liquid interface will deviate from the equilibrium value.
Key words:  partition ratio      temperature gradient      external force field     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/130

1 Wood R F. Phys Rev B, 1982; 25: 2786
2 Jackson K A, Gilmer G H, Leamy H J. In: White C W, Peercy P S eds., Laser and Electron Beam Processing of Materials, New York: Academic, 1980: 104
3 Aziz M J. J Appl Phys. 1982; 53: 1158
4 李如生,非平衡态热力学和耗散结构,北京:清华大学出版社,1986:105
5 下地光雄著,郭淦钦译,液态金属,科学出版社,1987:275
[1] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[2] CUI Hongbao; GUO Jingjie; BI Weisheng; SU Yanqing; WU Shiping; FU Hengzhi. THE EVOLUTION OF UNIDIRECTIONAL SOLIDIFI-CATION MICROSTRUCTURE OF THE Al-In MONOTECTIC ALLOYS IN HIGH TEMPERATURE GRADIENT[J]. 金属学报, 2004, 40(12): 1253-1256 .
[3] TANG Zhonghe;GUO Shangxing;CHEN Yongding Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. EQUILIBRATING PARTITION RATIOS OF Nb, Mn and Si BETWEEN LIQUID IRON AND MgO-SiO_2 -MnO SLAG MELTS[J]. 金属学报, 1988, 24(5): 397-402.
No Suggested Reading articles found!