Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (1): 113-119    DOI:
Current Issue | Archive | Adv Search |
KINETIC STUDY OF DESULPHURIZATION ALONG METAL-SLAG INTERFACE
JIANG Guochang;XU Kuangdi;DENG Jianxiong Shanghai University of Technology GUO Zhancheng; GUAN Yulong University of Science and Technology Beijing Institute of Metallurgy and Materials;Shanghai University of Technology; Shanghai 200072
Cite this article: 

JIANG Guochang;XU Kuangdi;DENG Jianxiong Shanghai University of Technology GUO Zhancheng; GUAN Yulong University of Science and Technology Beijing Institute of Metallurgy and Materials;Shanghai University of Technology; Shanghai 200072. KINETIC STUDY OF DESULPHURIZATION ALONG METAL-SLAG INTERFACE. Acta Metall Sin, 1990, 26(1): 113-119.

Download:  PDF(481KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An electrochemical model, directly deduced from the principle of elec-trochemistry, together with the calculational method for initial oxygen potentialalong the metal-slag interface may be available to quantitatively describe the plotof %S vs time. It was found that during desulphurization both the distribution con-stant of S along metal-slag interface, L_S~*, and distribation index inside the bulk,L'_S, vary with the descending of oxygen potential along metal-slag interface. Butthe plot of L_S~* vs time is quite different from L'_S vs time, being of parabola or hy-perhola type respectively. The variation of the driving force parameter vs time,obtained either calculated or experimental, plotted as a camel hump.
Key words:  desulphurization      metal-slag interface      electrochemical model     
Received:  18 January 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I1/113

1 Deng Jianxiong (邓健雄), Oeters F. Preprints of 7th Japan-Germany Seminar on Fundamenials of Iron and Steel Making, Duesseldorf, 1987
2 Wagner C. In: Elliot J F ed, The Physical Chemistry of Steelmaking, New York: John Wiley, 1958: 237--251
3 PluscMell S W, Dortmund B R, Schuermann E. Arch Eisenhuettenwes, 1981: 52 (3) : 85--89
4 Riboud P P, Olette M. Proc 7th Int on Vacuum Metallurgy, Vol. II, Tokyo: The Iron Steel Inst of Japan, 1982: 879--889
5 Adamson A W,顾惕人译,表面的物理化学,北京:科学出版社,1984:151
6 Bard A J,Faulkner L R.谷林瑛等译.电化学方法(原理及应用),北京:化学工业出版社,1986:195
7 田昭武.电化学研究方法,北京:科学出版社,1984:24
8 Nicholson A, Howarth D J, Turton J. Ironmaking Steelmaking, 1983; 10: 31--45k
[1] WEI Chiho;ZHU Shoujun; YU Nengwen (Shanghai Enhanced Laboratory of Ferrous Metallurgy; Shanghai University; Shanghai 200072). KINETICS OF DESULPHURIZATION BY POWDER INJECTION AND BLOWING IN RH REFINING OF MOLTEN STEEL[J]. 金属学报, 1998, 34(5): 497-505.