| KINETIC STUDY OF DESULPHURIZATION ALONG METAL-SLAG INTERFACE |
| JIANG Guochang;XU Kuangdi;DENG Jianxiong Shanghai University of Technology GUO Zhancheng; GUAN Yulong University of Science and Technology Beijing Institute of Metallurgy and Materials;Shanghai University of Technology; Shanghai 200072 |
|
Cite this article:
JIANG Guochang;XU Kuangdi;DENG Jianxiong Shanghai University of Technology GUO Zhancheng; GUAN Yulong University of Science and Technology Beijing Institute of Metallurgy and Materials;Shanghai University of Technology; Shanghai 200072. KINETIC STUDY OF DESULPHURIZATION ALONG METAL-SLAG INTERFACE. Acta Metall Sin, 1990, 26(1): 113-119.
|
|
|
Abstract An electrochemical model, directly deduced from the principle of elec-trochemistry, together with the calculational method for initial oxygen potentialalong the metal-slag interface may be available to quantitatively describe the plotof %S vs time. It was found that during desulphurization both the distribution con-stant of S along metal-slag interface, L_S~*, and distribation index inside the bulk,L'_S, vary with the descending of oxygen potential along metal-slag interface. Butthe plot of L_S~* vs time is quite different from L'_S vs time, being of parabola or hy-perhola type respectively. The variation of the driving force parameter vs time,obtained either calculated or experimental, plotted as a camel hump.
|
|
Received: 18 January 1990
|
1 Deng Jianxiong (邓健雄), Oeters F. Preprints of 7th Japan-Germany Seminar on Fundamenials of Iron and Steel Making, Duesseldorf, 1987 2 Wagner C. In: Elliot J F ed, The Physical Chemistry of Steelmaking, New York: John Wiley, 1958: 237--251 3 PluscMell S W, Dortmund B R, Schuermann E. Arch Eisenhuettenwes, 1981: 52 (3) : 85--89 4 Riboud P P, Olette M. Proc 7th Int on Vacuum Metallurgy, Vol. II, Tokyo: The Iron Steel Inst of Japan, 1982: 879--889 5 Adamson A W,顾惕人译,表面的物理化学,北京:科学出版社,1984:151 6 Bard A J,Faulkner L R.谷林瑛等译.电化学方法(原理及应用),北京:化学工业出版社,1986:195 7 田昭武.电化学研究方法,北京:科学出版社,1984:24 8 Nicholson A, Howarth D J, Turton J. Ironmaking Steelmaking, 1983; 10: 31--45k |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|