| KINETIC EQUATIONS WITH VARIATION OF LIQUID REACTANT CONCENTRATION |
| YIN Qunsheng;ZHAO Tiancong;ZHONG Tingke;LIN Ruoya Central South University of Techology; Changsha Department of Metallurgy;Central South University of Technology; Changsha 410083 |
|
Cite this article:
YIN Qunsheng;ZHAO Tiancong;ZHONG Tingke;LIN Ruoya Central South University of Techology; Changsha Department of Metallurgy;Central South University of Technology; Changsha 410083. KINETIC EQUATIONS WITH VARIATION OF LIQUID REACTANT CONCENTRATION. Acta Metall Sin, 1990, 26(1): 120-127.
|
|
|
Abstract For two common types of liquid-solid heterogeneous reactions, thekinetic eqtiations have been established which involved both the variation of liquidreactant concentration and the variation of solid reactant geometry with thereaction time. The experimental results show that the kinetic equations are moreaccurate and reasonable than those appeared in previous literatures. Moreover, theyare also suitable for gas-solid heterogeneous reactions in principle.
|
|
Received: 18 January 1990
|
1 Wadsworth M E. In: Hong Yong Sohn, Wadsworth M E eds., Rate Processes of Extractive Metallurgy, New York: Plenum Press, 1979: 150 2 #12 3 Kanome O. Abe H, Okuwaki A, Okabe T. Hydrometallurgy, 1987; 19 (1) : 1 4 殷群生.中南工业大学博士学位论文,1987 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|