Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (1): 151-152    DOI:
Current Issue | Archive | Adv Search |
NODULARIZATION OF CARBIDE IN AS-CAST WEAR-RESISTANT MANGANESE STEEL
JIANG Qichuan;HE Zhenming;YAN Jiulin;CUI Donghuan;WANG Shoushi Jilin University of Technology; Changchun Associate Professor;Faculty of Cast; Jilin University of Technology; Changchun 130025
Cite this article: 

JIANG Qichuan;HE Zhenming;YAN Jiulin;CUI Donghuan;WANG Shoushi Jilin University of Technology; Changchun Associate Professor;Faculty of Cast; Jilin University of Technology; Changchun 130025. NODULARIZATION OF CARBIDE IN AS-CAST WEAR-RESISTANT MANGANESE STEEL. Acta Metall Sin, 1990, 26(1): 151-152.

Download:  PDF(828KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The needle-like and network carbides in wear-resistant high carbon manganesesteel as-casted will be nodularized and dispersed. by a large majority, in austenite after modi-fication with Mg system agents. The impact toughness of the steels may be obviously improvedand the hardness also increased to a certain extent. And therefore it seems to be available whenthe steels are still as-casted, and no necessity of heat treatment may be often made to bettertheir wear resistance.
Key words:  Mg modified      as-cast manganese steel      nodularized carbide     
Received:  18 January 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I1/151

[1] JIANG Qichuan;LI Zhang;WANG Shoushi;HE Zhenming Jilin University of Technology; Changchun associate professor;Faculty of foundary Jilin University of Technology;Changchun 130025. BEHAVIOUR OF Ti IN AS-CAST MEDIUM MANGANESE AUSTENITIC STEEL[J]. 金属学报, 1990, 26(4): 130-134.
No Suggested Reading articles found!