Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (3): 126-130    DOI:
Current Issue | Archive | Adv Search |
COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER
LIU Yansheng;ZHAO Xiong;LIANG Zhide Northeast University of Technology; Shenyang Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006
Cite this article: 

LIU Yansheng;ZHAO Xiong;LIANG Zhide Northeast University of Technology; Shenyang Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006. COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER. Acta Metall Sin, 1990, 26(3): 126-130.

Download:  PDF(409KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The texture change along the normal direction to rolling plane ofcross shear rolled commercial copper has been studied by means of the two-stepmethod for ODF calculation and computer simulation. The texture of cross shearrolling of copper is similar in primary components to that of conventional coldrolling, but the scattering degree and direction of the texture are different due to theresidual shear strain change in different position along the normal to rolling plane.It seems that no more effect of the shear strain upon the recrystallization texture.
Key words:  cross shear rolling      cold rolled texture      recrystallization texture      texture simulation     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/126

1 朱泉.钢铁,1980;15:1
2 梁志德,徐家桢,王福.织构材料的三继取向分析术,沈阳:东北工学院出版社,1986:108
3 Taylor G I. J Inst Met. 1938; 62: 307
4 Houtte P V, Aernoudt E. Z Metallk. 1975; 66: 202
5 刘燕声,梁志德.科学通报,1989;6:471]
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] Quan FU,Yuhui SHA,Zhenghua HE,Fan LEI,Fang ZHANG,Liang ZUO. Recrystallization Texture and Magnetostriction in Binary Fe81Ga19 Sheets[J]. 金属学报, 2017, 53(1): 90-96.
[3] Yan ZHANG,Mingxing GUO,Hui XING,Fei WANG,Xiaofeng WANG,Jishan ZHANG,Linzhong ZHUANG. INFLUENCE OF DIFFERENT THERMOMECHANICAL PROCESSES ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF Al-Mg-Si-Cu ALLOY SHEETS[J]. 金属学报, 2015, 51(12): 1425-1434.
[4] Xiang Zhao. EFFECTS OF ELECTRIC FIELD ANNEALING ON PLASTIC STRAIN RATIO (r VALUE) OF IF STEEL SHEET[J]. 金属学报, 2006, 42(8): 827-829 .
[5] HUANG Tao; QU Jiahui; HU Zhuochao; WANG Fu; ZUO Liang. EVOLUTION OF THE ORIENTATION OF CROSS SHEAR ROLLING HIGH PURITY ALUMINUM FOILS DURING DEFORMATION AND RECRYSTALLIZATION[J]. 金属学报, 2005, 41(9): 953-957 .
[6] LÜ Aiqiang; ZHANG Yang; LI Ying; LIU Gang; LIU Chunming. Effect of cross shear rolling on microstructure and properties of surface nanocrystallized 316L stainless steel[J]. 金属学报, 2005, 41(3): 271-276 .
[7] YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel: (010)62333436; Fax: (010)62332336. PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture[J]. 金属学报, 1998, 34(8): 793-801.
[8] YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel. (010)623s3Js6; Fax: (010)62332336. PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RECRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅰ. Deformation Zones Around Particles and Particle Stimulated Nucleation[J]. 金属学报, 1998, 34(8): 785-792.
[9] LIU Gang (School of Materials and Metallurgy; Northeastern University; Shenyang 110006; School of Chemical Science and Engineering; Liaoning University; Shenyang 110036)QI Kemin; WANG Fu; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). THE INFLUENCE OF MISMATCH SPEED RATIO ON TEXTURE DEVELOPMENT IN CROSS SHEAR ROLLED 3% SILICON STEEL[J]. 金属学报, 1998, 34(4): 400-405.
[10] LIU Gang (Northeastern University; Shenyang 110006; Liaoning University);Shenyang 110036); WANG Fu; QI Kemin;;LIU Guilan; LIANG Zhide (Northeastern University; Shenyang 110006)(Manuscript received 1996-03-20; in revised form 1996-07-10). TEXTURE DISTRIBUTION AND DEVELOPMENT THROUGH THE THICKNESS AFTER CROSS SHEAR ROLLING OF GRAIN ORIENTED SILICON STEEL[J]. 金属学报, 1997, 33(4): 364-369.
[11] ZHAO Xiang(Northeastern University; Shenyang 110006); SEKI Fumie; ITO Kunio(Universily of Tokyo; Japon); YOSHINADA Naoki(Nippon Steel Compony; Japan) (Manuscript received 1994-03-07; in revised form 1995-01-12). INFLUENCE OF DISSOLVED CARBON CONTENT ON RECRYSTALLIZATION γ TEXTURE IN ULTRA-LOW CARBON DEEP DRAWING STEEL WITH HIGH PURITY[J]. 金属学报, 1995, 31(18): 262-265.
[12] ZHANG Yumei;JIANG Wenhui Northeast University of Technology; ShenyangDept.of Materials Science and Engineering;Northeast University of Technology;Shenyang. SECONDARY RECRYSTALLIZATION TEXTURE IN 50%Ni-Fe ALLOY WITH CUBIC ORIENTATION[J]. 金属学报, 1988, 24(3): 217-220.
No Suggested Reading articles found!