Abstract The diagram of srstem AU-Cu-Si was constructed from data of 9 internal sectionsby DTA in an atmosphere of dry N_2. The composition of ternary eutectic point melting at337℃ lies in Au(74.7)-Cu(6.1)-Si(19.2) at.-%. The liquidus of the 3 side-binary systems havebeen redetermined.
|
|