Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (4): 153-154    DOI:
Current Issue | Archive | Adv Search |
LIQUIDUS OF Au-Cu-Si SYSTEM
LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing
Cite this article: 

LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing. LIQUIDUS OF Au-Cu-Si SYSTEM. Acta Metall Sin, 1990, 26(4): 153-154.

Download:  PDF(103KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The diagram of srstem AU-Cu-Si was constructed from data of 9 internal sectionsby DTA in an atmosphere of dry N_2. The composition of ternary eutectic point melting at337℃ lies in Au(74.7)-Cu(6.1)-Si(19.2) at.-%. The liquidus of the 3 side-binary systems havebeen redetermined.
Key words:  Au-Cu-Si system      liquidus      DTA     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/153

1 Massalski T B. Binary Alloy Phase Diagrams, Metals Park, Ohio: ASM, 1986: 254, 313, 960
2 刘淑祺,孙文庆.金属学报,1988;24:B376
[1] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[2] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[3] XING Pengfei; ZHAI Yuchun; TIAN Yanwen; GENG Yan; CHEN Feng(Northeastern University; Shenyang 110006)(Manuscript received 1995-04-24; in revised form 1995-10-16). STUDY ON THE OXIDATION KINETICS OF WS_2 IN OPEN AIR[J]. 金属学报, 1996, 32(2): 187-190.
[4] WEI Jihe (Shanghai Univereity.of Technology);LIU Zongyuan(Xi'van Institute of Metallurgy Construction Engineering). STUDY ON OXYGEN TRANSFER THROUGH MOLTEN SLAGS OF CaF_2+Al_2O_3 AND CaF_2+Al_2O_3+CaO SYSTEMS FOR ESR[J]. 金属学报, 1994, 30(20): 350-360.
[5] LIU Shuqi;YI Tao Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Ge PHASE DIAGRAM[J]. 金属学报, 1989, 25(2): 155-156.
[6] ZHENG Chaogui;JIN Jun;YE Yupu Peking University. LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM[J]. 金属学报, 1989, 25(1): 147-149.
[7] QIU Yiming;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. RULE OF SEGREGATION OF ALLOYING ELEMENTS IN CAST Ni-BASE SUPERALLOYS[J]. 金属学报, 1989, 25(1): 78-80.
[8] LIU Shuqi;SUN Wenqing Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Bi SYSTEM[J]. 金属学报, 1988, 24(5): 448-450.
No Suggested Reading articles found!