| EFFECT OF HYDROGEN ON DEBYE TEMPERATURE AND LATTICE PARAMETER OF TITANIUM ALLOY |
| YU Bingxi;GAO Shujun Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
YU Bingxi;GAO Shujun Institute of Metal Research; Academia Sinica; Shenyang. EFFECT OF HYDROGEN ON DEBYE TEMPERATURE AND LATTICE PARAMETER OF TITANIUM ALLOY. Acta Metall Sin, 1990, 26(6): 29-33.
|
|
|
Abstract The variations of Debye temperature and lattice parameter of a Ti-30Mo alloy with different hydrogen contents have been measured by means of X-raydiffraction. It was found that as the hydrogen content increases, the Debye tempe-rature decreases, but the lattice parameter of the alloy is increased. The above res-ults support experimentally the decohesion theory that hydrogen in metals willweaken the cohesive force between the atoms and make metals brittle.
|
|
Received: 18 June 1990
|
1 Oriani R A, Josephic P H. Acta Metall, 1974; 22: 1065 2 张统一,蒋方忻,褚武扬,肖纪美.金属学报,1987;23:A 457 3 高佩玉.中国腐蚀与防护学报,1982;2(3) :10 4 Lipson H. In: Kasper J S, Lonsdale K eds., International Tables for X-ray Crystallography, Vol. Ⅱ, Birmingham, England: The Kynoch Press, 1972: 264 5 李鹏兴.见:徐祖耀,李鹏兴主编,材料科学导论.上海科学技术出版社,1986:74g |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|