| TRANSFORMATION HYSTERESIS AND STABILITYOF STRAIN MARTENSITE IN Ni_(47)Ti_(44)Nb_9 ALLOY |
| ZHANG Chunsheng;CAI Wei;ZHAO Liancheng (Harbin Institute of Technology |
|
Cite this article:
ZHANG Chunsheng;CAI Wei;ZHAO Liancheng (Harbin Institute of Technology. TRANSFORMATION HYSTERESIS AND STABILITYOF STRAIN MARTENSITE IN Ni_(47)Ti_(44)Nb_9 ALLOY. Acta Metall Sin, 1991, 27(3): 51-55.
|
|
|
Abstract The transformation hysteresis and stability of strain martensite inNi_(47)Ti_(44)Nb_9 alloy have been studied by means of tensile test under various temper-atures, electrical resistance measurement and TEM observation. It was shown thatthere is a characteristic deformation temperature and a strain range, in which thecritical yield stress for stress-induced transformation acquires optimum matchingwith the yield strength of the β-Nb particles. In this case, deformation effectivelyincreases the transformation hysteresis, while the strain recovery ratio remains use-fully high. The martensite with irregular fine twin substructure and martensitecontaining some dislocations as well as martensite intersected by the β-Nb particlespossess high stability.
|
|
Received: 18 March 1991
|
1 Zhao L C, Duerig T W. Wayman C M. Proc of the MRS Int Meeting on Advanced Materials, Vol. 9, 1988: 171 2 Zhao L C, Duerig T W, Just S, Melton K N, Proft J L, Yu W, Wayman C M. Scr Metall, 1990; 24: 221 3 Zhang C S, Zhao L C, Duerig T W, Wayman C M. Scr Metall, 1990; 24: 1807 4 Warlimont H et al. J Mater Sci, 1974; 9: 1545 5 Mohamed H A, Washburn J. Metall Trans, 1976; 7A: 1041 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|