| INFLUENCE OF DISPERSED γ′ ECIPITATEDPARTICLES ON MARTENSITE MORPHOLOGY IN Fe-Ni Co-Ti ALLOYS |
| CUI Lishan Jinzhou Institute of Technology; YANG Dazhi; LI Guobin ZHU Min Dalian University of Technology |
|
Cite this article:
CUI Lishan Jinzhou Institute of Technology; YANG Dazhi; LI Guobin ZHU Min Dalian University of Technology. INFLUENCE OF DISPERSED γ′ ECIPITATEDPARTICLES ON MARTENSITE MORPHOLOGY IN Fe-Ni Co-Ti ALLOYS. Acta Metall Sin, 1991, 27(3): 46-50.
|
|
|
Abstract The martensite is featured as thin plate when the γ′dispersed precipi-tated particles are the size of about 20--50 nm formed at low temperature in Fe-iN-Oo-Ti alloys. The interface of martensite plate is not smooth. If the γ′particlesare sized less than 5 nm, the thin plate martensite with thermoelasticity may befound at low temperature, while greater than 5 nm, the intermittent martensite mayoccur, and increase both in size and quantity with the coarsening of the γ′parti-cles. The lenticular or butterfly martensite is formed at low temperature until theγ′particles up to 10--15 nm.
|
|
Received: 18 March 1991
|
1 Maki T, Kobayashi K, Minato M. Scr Metall, 1984; 18: 1105 2 Maki T, Kobayashi K, Tamura I. Proc Int Conf on Martensitic Transformations, (ICOMAT-82) , Leuven, Belgium, 1982: C4--541 3 Gunko L P, Koval Y N, Kozlova L Y, Kokorin V V, Osipenko I A. Phys Met Metall, 1982; 53(2) : 114, 118 4 Neuhauser H J, Pitsch W. Acta Metall, 1971; 19: 337 5 Patterson R L, Wayman C M. Acta Metall, 1964; 12: 1306; 1966; 14: 374 6 Reed R P. Acta Metall, 1967; 15: 1287 7 Maki T, Shimooka S. Umemoto M. Trans Jpn Inst Met, 1972; 13: 400 8 Fearon E O, Bevis M. Acta Metall. 1974; 22: 991 9 Miner R E. Metall Trans, 1971: 2: 1250 10 Maki T, Wayman C M. Acta Metall, 1977; 25: 695, 710 |