A THERMAL ANALYSIS STUDY OF Fe-Cr-Mn HEAT RESISTANT ALLOY
LIANG Gongying;XING Jiandong Xi'an Jiaotong University
Cite this article:
LIANG Gongying;XING Jiandong Xi'an Jiaotong University. A THERMAL ANALYSIS STUDY OF Fe-Cr-Mn HEAT RESISTANT ALLOY. Acta Metall Sin, 1991, 27(6): 99-103.
Abstract Thermal analysis has been adopted to determine the liquidus and eutectic temperature of Fe-20% Cr-Mn alloy over range of Mn and C contents. Using regression analysis, the partial quasi-binary phase diagrams of Fe-Mn alloy (solidification range) have been constructed. And the effect of Mn content on liquidus and eutectic temperature was discussed.
中井弘,市场幹之,岡田健.日本金属学会志,1988;52:57--64 2 陆文华主编.铸铁及其熔炼.北京:机械工业出版社,1981:45 3 Arnald B K, Sare I R. A Thermal Analysis Study of Alloy White Cast Irons, The Foundymen, Augest/September, 1987: 330--335 4 侯增寿,陶岚琴.实用三元相图.上海:上海科学技术出版社,1982:105
WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES[J]. 金属学报, 1998, 34(9): 992-998.