Abstract Thermal analysis has been adopted to determine the liquidus and eutectic temperature of Fe-20% Cr-Mn alloy over range of Mn and C contents. Using regression analysis, the partial quasi-binary phase diagrams of Fe-Mn alloy (solidification range) have been constructed. And the effect of Mn content on liquidus and eutectic temperature was discussed.
|