PHASE DIAGRAM OF KF-LiCl-SrCl_2 SYSTEM |
YAN Licheng; XU Jingyan; YANG Jinxiu; DING Yong (Shanghai University of Science and Technology) |
|
Cite this article:
YAN Licheng; XU Jingyan; YANG Jinxiu; DING Yong (Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-SrCl_2 SYSTEM. Acta Metall Sin, 1992, 28(11): 62-64.
|
Abstract Phase dingram of KF-LiCl-SrCl2 system has been determined by visual variable-temperature methed. Its functional relation of the parameter of solution energy vs area of rigion of the primary divalent metal fluoride crystal, proposed by the authors previously, has also been discussed.
|