LAMELLAR MICROSTRUCTURE IN DUPLEX Ti-Al-V INTERMETALLIC COMPOUND |
GAO Ying;ZHU Jing;CAI Qigong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing |
|
Cite this article:
GAO Ying;ZHU Jing;CAI Qigong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. LAMELLAR MICROSTRUCTURE IN DUPLEX Ti-Al-V INTERMETALLIC COMPOUND. Acta Metall Sin, 1992, 28(2): 14-18.
|
Abstract The morphology and crystallographic orientation of (a_2+γ) lamellar structure in duplex Ti--47.5Al--2.5V intermetallic compound have been studied by means of TEM,microdiffraction as well as 180°and non--180° rotation twinning analysis. A possible atomic model of the interface was suggested. Thus, approach was made to a mechanism on complex nucleation of α_2+γ two phases along α--Ti interface, and growth of α_2/γ/γ_t/α_2 or α_2/γ/α_2/γ as fundamental structural unit.
|
Received: 18 February 1992
|
1 Lipsitt H A, Shechtman D, Schafrik R E. Metall Trans, 1975; 6A: 1991 2 Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 299 3 Hall E L, Huang Shyh-Chin. J Mater Res, 1989; 4: 595 4 Blackburn M J, Smith M P. U S Pat, 4 292 615, 1981 5 Blackburn M J. In: Jaffee R I, Promisel N E eds., The Science, Technology and Application of Titanium. Proc Int Conf, London, 21--24 May, 1968, London: Pergamon Press, 1970: 633 6 Feng C R, Michel D J. Crowe C R. Scr Metall, 1988; 22: 1481 7 Feng C R. Scr Metall, 1989; 23: 1135 8 高颖,朱静.电子显微学报,待发表 9 Swartz D S, Sastry S M L. Scr Metall, 1989; 23: 1621 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|